Influence of Post-Weld Heat Treatments on the Hydrogen Embrittlement Susceptibility of API 5L X52N Pipeline Steel Welded Joints
This work evaluates the influence of post-weld heat treatments (PWHT) on the hydrogen embrittlement (HE) susceptibility of girth-welded API 5L X52N pipeline steels. Four conditions were analyzed: as-welded, two stress-relief treatments (HT1 at 635.1 °C and HT3 at 593.5 °C), and a normalizing treatment (HT2 at 911.4 °C). Mechanical characterization was performed via Slow Strain Rate Tests (SSRT) in high-pressure hydrogen (160 bar) and air. Normalizing (HT2) homogenized the joint microstructure and increased plastic elongation in air and hydrogen; however, it produced the lowest reduction-of-area retention among the cross-weld conditions (HEIRA = 0.57), indicating greater hydrogen sensitivity during localized final fracture, while its plastic-elongation retention remained comparable to the as-welded condition. Among stress-relief treatments, HT1 showed the most favorable ductility retention in the filler metal, although this observation rests on a single FM-fractured specimen per condition and is not statistically conclusive. Fractographic analysis revealed a transition from ductile dimples in air to mixed-mode fracture in hydrogen, characterized by transgranular quasi-cleavage. The study suggests that acicular ferrite in the filler metal offers greater resistance to hydrogen-induced crack propagation than the equiaxed polygonal-ferrite microstructure produced by normalizing.
Authors
- Nevena Marinova (ORCID: https://orcid.org/0000-0002-3055-6267)
- Unai De Francisco (ORCID: https://orcid.org/0000-0002-2130-1721)
- Pablo Benguria (ORCID: https://orcid.org/0000-0001-8189-1412)
- Nora Guenaga Gomez
Institutions
- Tecnalia (ES)
Publication Details
- Journal
- Metals
- Published
- 2026-11-27
- DOI
- https://doi.org/10.3390/met16121303
- Primary Topic
- Hydrogen embrittlement and corrosion behaviors in metals
- Type
- article
- Field-Weighted Citation Impact
- 0.00