Effect of Prolonged Self-Etching Ceramic Primer Application and Reaction Protocols on Surface Characteristics and Shear Bond Strength of CAD/CAM Ceramics: An In Vitro Study

This study evaluated the effects of prolonged self-etching ceramic primer protocols on surface roughness (Ra), topography, shear bond strength (SBS), and failure modes of three CAD/CAM ceramics. Lithium disilicate (IPS e.max CAD), advanced lithium disilicate (CEREC Tessera), and feldspathic ceramic (VITABLOCS Mark II) specimens received hydrofluoric acid etching plus silane (HF+S) or Monobond Etch & Prime (MEP). For MEP, active application and passive reaction times were increased together using paired durations of 20/40, 40/80, or 60/120 s, respectively (n = 10 per group). Ra was measured by optical profilometry, and additional specimens underwent qualitative scanning electron microscopy. SBS was measured after 10,000 thermocycles, followed by failure-mode classification. Ra and SBS were analyzed using two-way ANOVA and Tukey’s HSD; failure modes were analyzed using the Fisher–Freeman–Halton test. Ceramic material, treatment, and their interaction significantly affected Ra and SBS (p < 0.001). For both lithium disilicate-based ceramics, SBS did not differ significantly between MEP 40/80 s and HF+S, whereas MEP 60/120 s produced significantly higher SBS than HF+S. HF+S produced the highest SBS for feldspathic ceramic. Failure-mode distributions differed across the material–treatment groups (p < 0.001). Under the tested laboratory conditions, the combined 60/120 s MEP protocol produced higher SBS after thermocycling than HF+S for the two lithium disilicate-based ceramics, whereas HF+S produced the highest SBS for the feldspathic ceramic.

Authors

Institutions

Publication Details

Journal
Bioengineering
Published
2026-11-27
DOI
https://doi.org/10.3390/bioengineering13121453
Primary Topic
Dental materials and restorations
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effect of Prolonged Self-Etching Ceramic Primer Application and Reaction Protocols on Surface Characteristics and Shear Bond Strength of CAD/CAM Ceramics: An In Vitro Study

Hessa AlOtaibi, Ahmed M. Maawadh, Thamer Almohareb, Ayman M. Sulimany
Bioengineering
Dental materials and restorations
article

Effect of Prolonged Self-Etching Ceramic Primer Application and Reaction Protocols on Surface Characteristics and Shear Bond Strength of CAD/CAM Ceramics: An In Vitro Study

Hessa AlOtaibi, Ahmed M. Maawadh, Thamer Almohareb, Ayman M. Sulimany
article en

Abstract

This study evaluated the effects of prolonged self-etching ceramic primer protocols on surface roughness (Ra), topography, shear bond strength (SBS), and failure modes of three CAD/CAM ceramics. Lithium disilicate (IPS e.max CAD), advanced lithium disilicate (CEREC Tessera), and feldspathic ceramic (VITABLOCS Mark II) specimens received hydrofluoric acid etching plus silane (HF+S) or Monobond Etch & Prime (MEP). For MEP, active application and passive reaction times were increased together using paired durations of 20/40, 40/80, or 60/120 s, respectively (n = 10 per group). Ra was measured by optical profilometry, and additional specimens underwent qualitative scanning electron microscopy. SBS was measured after 10,000 thermocycles, followed by failure-mode classification. Ra and SBS were analyzed using two-way ANOVA and Tukey’s HSD; failure modes were analyzed using the Fisher–Freeman–Halton test. Ceramic material, treatment, and their interaction significantly affected Ra and SBS (p < 0.001). For both lithium disilicate-based ceramics, SBS did not differ significantly between MEP 40/80 s and HF+S, whereas MEP 60/120 s produced significantly higher SBS than HF+S. HF+S produced the highest SBS for feldspathic ceramic. Failure-mode distributions differed across the material–treatment groups (p < 0.001). Under the tested laboratory conditions, the combined 60/120 s MEP protocol produced higher SBS after thermocycling than HF+S for the two lithium disilicate-based ceramics, whereas HF+S produced the highest SBS for the feldspathic ceramic.

BioengineeringVol. 13(12)
King Saud University (SA)
Dental materials and restorations
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
Effect of Prolonged Self-Etching Ceramic Primer Application and Reaction Protocols on Surface Characteristics and Shear Bond Strength of CAD/CAM Ceramics: An In Vitro Study — Hessa AlOtaibi, Ahmed M. Maawadh, et al. · Bioengineering (2026) | TGRS Research Map | TGRS