Wear and corrosion behavior of surface-treated Ti6Al4V via electro-spark deposition using a zirconium electrode to form super-hard ceramic-based coatings

The present study investigates the microstructural evolution, tribological properties, hardness response, and corrosion resistance of zirconium-based coatings deposited on biomedical Ti6Al4V-ELI alloy via the electro-spark deposition (ESD) process. The results demonstrate that increasing ESD input energy significantly enhances coating thickness up to 80.3 µm but concurrently promotes the formation of detrimental microcracks, particularly under the highest energy condition (75 V/280 µF), where the tetragonal-to-monoclinic ZrO 2 phase transformation induces severe tensile stresses. XRD analysis confirmed that coating phase assemblages depend heavily on processing parameters: 50V/20µF formed ZrN, α-Zr, and Zr 4.76 Ti 7.24 O 2 ; 50/280 comprised TiN, ZrN, monoclinic ZrO 2 ​, and ZrTi; 75V/20 produced Ti 9 ​N 3.87 ​, ZrN, monoclinic ZrO 2 ​, and Zr 1.18 Ti 2.19 ; and 75/280 yielded TiN, ZrN, dual monoclinic/tetragonal ZrO 2 ​, and ZrTi. The maximum microhardness of 1946 HV and the lowest specific wear rate of 4.00 × 10 –4 mm 3 /(N.m) were achieved for the coating deposited at 50 V/280 µF, representing a 25% reduction in the mean specific wear rate relative to the bare substrate. The coating deposited at the lowest energy input (50V/20µF) exhibited a remarkable improvement in corrosion resistance compared to the bare substrate, achieving a polarization resistance of 1.07 × 10 6 Ω.cm², approximately 19.5 times that of the uncoated Ti6Al4V. This investigation demonstrates the capability of ESD in-situ formation of super-hard coatings with superior wear resistance or dense, defect-free layers for enhanced corrosion protection on biomedical titanium alloys.

Authors

Institutions

Publication Details

Journal
Applied Surface Science Advances
Published
2026-11-27
DOI
https://doi.org/10.1016/j.apsadv.2026.101112
Primary Topic
Surface Treatment and Coatings
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Wear and corrosion behavior of surface-treated Ti6Al4V via electro-spark deposition using a zirconium electrode to form super-hard ceramic-based coatings

Parvaneh Farshbaf, Farzad Habibi, Ahad Samadi, Fatemeh Najjar
Applied Surface Science Advances
Surface Treatment and Coatings
article

Wear and corrosion behavior of surface-treated Ti6Al4V via electro-spark deposition using a zirconium electrode to form super-hard ceramic-based coatings

Parvaneh Farshbaf, Farzad Habibi, Ahad Samadi, Fatemeh Najjar
article en

Abstract

The present study investigates the microstructural evolution, tribological properties, hardness response, and corrosion resistance of zirconium-based coatings deposited on biomedical Ti6Al4V-ELI alloy via the electro-spark deposition (ESD) process. The results demonstrate that increasing ESD input energy significantly enhances coating thickness up to 80.3 µm but concurrently promotes the formation of detrimental microcracks, particularly under the highest energy condition (75 V/280 µF), where the tetragonal-to-monoclinic ZrO 2 phase transformation induces severe tensile stresses. XRD analysis confirmed that coating phase assemblages depend heavily on processing parameters: 50V/20µF formed ZrN, α-Zr, and Zr 4.76 Ti 7.24 O 2 ; 50/280 comprised TiN, ZrN, monoclinic ZrO 2 ​, and ZrTi; 75V/20 produced Ti 9 ​N 3.87 ​, ZrN, monoclinic ZrO 2 ​, and Zr 1.18 Ti 2.19 ; and 75/280 yielded TiN, ZrN, dual monoclinic/tetragonal ZrO 2 ​, and ZrTi. The maximum microhardness of 1946 HV and the lowest specific wear rate of 4.00 × 10 –4 mm 3 /(N.m) were achieved for the coating deposited at 50 V/280 µF, representing a 25% reduction in the mean specific wear rate relative to the bare substrate. The coating deposited at the lowest energy input (50V/20µF) exhibited a remarkable improvement in corrosion resistance compared to the bare substrate, achieving a polarization resistance of 1.07 × 10 6 Ω.cm², approximately 19.5 times that of the uncoated Ti6Al4V. This investigation demonstrates the capability of ESD in-situ formation of super-hard coatings with superior wear resistance or dense, defect-free layers for enhanced corrosion protection on biomedical titanium alloys.

Applied Surface Science AdvancesVol. 36
Sahand University of Technology (IR)
Surface Treatment and Coatings
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon