Mechanical properties and damage constitutive model of coal gangue ceramsite concrete with different aggregate volume fractions

Amid the dual carbon strategy and solid waste resource utilization, lightweight concrete with coal gangue ceramsite as aggregate offers advantages, making research on its performance regulation and engineering application significant. This study adopted C90 coal gangue ceramsite concrete (CGCC) with varying ceramsite volume fractions as test samples. By uniaxial compression tests combined with the digital image correlation (DIC) method, it systematically explored the fraction's effects on CGCC mechanical behavior, failure modes, and energy evolution, and established a damage constitutive model taking ceramsite volume fraction as a parameter. Peak stress declines negatively with increasing ceramsite volume fraction, with a total reduction of 35.6%. Within 30–70% range, peak stress remains stable, accompanied by the highest average peak strain and smallest variance, achieving a synergistic balance between load-bearing capacity and deformation. Ceramsite fraction changes CGCC microstructure and shifts failure mode from diagonal shear to tension-shear mixed. DIC contour maps well reflected surface strain concentration and crack propagation. Total absorbed energy decreases and stabilizes after 60%, while dissipated energy rises by 67.4% in 60–100%, characterizing the enhanced ductility of CGCC specimens with high ceramsite volume fractions. Based on Weibull distribution and damage mechanics, the model with initial and load-induced damage variables agrees well with experimental data, describing mechanical responses of varying ceramsite volume fractions. This study provides theoretical support for engineering design and references for coal gangue utilization and low-carbon development of construction.

Authors

Institutions

Publication Details

Journal
International Journal of Damage Mechanics
Published
2026-11-27
DOI
https://doi.org/10.1177/10567895261505254
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Mechanical properties and damage constitutive model of coal gangue ceramsite concrete with different aggregate volume fractions

Yao Bai, Renliang Shan, Dongxu Sun, Xiao Tong et al.
International Journal of Damage Mechanics
Concrete and Cement Materials Research
article

Mechanical properties and damage constitutive model of coal gangue ceramsite concrete with different aggregate volume fractions

Yao Bai, Renliang Shan, Dongxu Sun, Xiao Tong, Zhenyu Xu, Tianyu Han, Haoyuan Liu
article en

Abstract

Amid the dual carbon strategy and solid waste resource utilization, lightweight concrete with coal gangue ceramsite as aggregate offers advantages, making research on its performance regulation and engineering application significant. This study adopted C90 coal gangue ceramsite concrete (CGCC) with varying ceramsite volume fractions as test samples. By uniaxial compression tests combined with the digital image correlation (DIC) method, it systematically explored the fraction's effects on CGCC mechanical behavior, failure modes, and energy evolution, and established a damage constitutive model taking ceramsite volume fraction as a parameter. Peak stress declines negatively with increasing ceramsite volume fraction, with a total reduction of 35.6%. Within 30–70% range, peak stress remains stable, accompanied by the highest average peak strain and smallest variance, achieving a synergistic balance between load-bearing capacity and deformation. Ceramsite fraction changes CGCC microstructure and shifts failure mode from diagonal shear to tension-shear mixed. DIC contour maps well reflected surface strain concentration and crack propagation. Total absorbed energy decreases and stabilizes after 60%, while dissipated energy rises by 67.4% in 60–100%, characterizing the enhanced ductility of CGCC specimens with high ceramsite volume fractions. Based on Weibull distribution and damage mechanics, the model with initial and load-induced damage variables agrees well with experimental data, describing mechanical responses of varying ceramsite volume fractions. This study provides theoretical support for engineering design and references for coal gangue utilization and low-carbon development of construction.

International Journal of Damage Mechanics
Hebei University of Engineering (CN), China University of Mining and Technology - Beijing (CN)
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon