Compression behavior of steel‐ PVA high‐strength self‐compacting concrete short column exposed to elevated temperatures

To investigate the post‐fire mechanical behavior of high‐strength self‐compacting concrete (HSSCC) short columns reinforced with steel‐polyvinyl alcohol (S‐PVA) hybrid fibers, 45 short columns were subjected to elevated‐temperature exposure followed by axial static compression tests. The results show that, at temperatures up to 400°C, the columns exhibited brittle axial‐compression failure. With increasing temperature, the residual load‐bearing capacity of all specimens first increased and then decreased, whereas the ductility coefficient initially decreased and subsequently increased. S‐PVA hybrid fibers improved post‐failure integrity and enhanced the residual load‐bearing capacity and ductility both at ambient temperature and after elevated‐temperature exposure. Within the dosage range investigated, SCC short columns containing 0.1 vol% PVA fiber and 1.4 vol% steel fiber exhibited superior post‐heating mechanical performance. Based on Chinese design‐code equations, a residual load‐bearing‐capacity calculation method for reinforced S‐PVA‐SCC short columns after elevated‐temperature exposure was developed using curve fitting and temperature reduction factors.

Authors

Institutions

Publication Details

Journal
Structural Concrete
Published
2026-11-25
DOI
https://doi.org/10.1002/suco.70884
Primary Topic
Fire effects on concrete materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Compression behavior of steel‐ PVA high‐strength self‐compacting concrete short column exposed to elevated temperatures

Liangli Xiao, Zhao Yang, Chengxiang Xu, Tao Li et al.
Structural Concrete
Fire effects on concrete materials
article

Compression behavior of steel‐ PVA high‐strength self‐compacting concrete short column exposed to elevated temperatures

Liangli Xiao, Zhao Yang, Chengxiang Xu, Tao Li, Xinlong Kong
article en

Abstract

To investigate the post‐fire mechanical behavior of high‐strength self‐compacting concrete (HSSCC) short columns reinforced with steel‐polyvinyl alcohol (S‐PVA) hybrid fibers, 45 short columns were subjected to elevated‐temperature exposure followed by axial static compression tests. The results show that, at temperatures up to 400°C, the columns exhibited brittle axial‐compression failure. With increasing temperature, the residual load‐bearing capacity of all specimens first increased and then decreased, whereas the ductility coefficient initially decreased and subsequently increased. S‐PVA hybrid fibers improved post‐failure integrity and enhanced the residual load‐bearing capacity and ductility both at ambient temperature and after elevated‐temperature exposure. Within the dosage range investigated, SCC short columns containing 0.1 vol% PVA fiber and 1.4 vol% steel fiber exhibited superior post‐heating mechanical performance. Based on Chinese design‐code equations, a residual load‐bearing‐capacity calculation method for reinforced S‐PVA‐SCC short columns after elevated‐temperature exposure was developed using curve fitting and temperature reduction factors.

Structural Concrete
Wuhan University of Science and Technology (CN)
Fire effects on concrete materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines