Detector-Level Transport Regimes inPolyethylene/Aluminium Shieldingof Silicon Sensors under Photon,Electron, and Proton Irradiation

Shielding performance inferred from attenuation or nominal thickness can misrepresent the response of a finite semiconductor detector. This study uses Geant4 to map energy deposited in a silicon sensor of dimensions 20 mm × 20 mm × 0.5 mm behind polyethylene (PE) and PE–aluminium (PE–Al) shields under controlled photon, electron, and proton fields. Event-level scoring separates primary survival, residual entry energy, shield-generated secondaries, and finite shield coverage. The proton response was strongly non-monotonic near range-out: effective suppression occurred between 8–9 mm PE at 30 MeV and between 20–25 mm PE at 50 MeV, in agreement with NIST PSTAR projected ranges. For photons, short shield-to-sensor gaps increased silicon energy deposition, consistent with enhanced acceptance of shield-generated secondaries. At the final 100 mm gap, adding 0.5 mm Al to 25 mm PE improved the photon-response reduction by 3.083 ± 0.558 percentage points under the reference physics list; the uncertainty is a two-sided 95% sampling confidence-interval half-width and excludes physics-model uncertainty. An XCOM narrow-beam calculation gave 1.01 percentage points of additional uncollided primary-photon number removal, a different observable that cannot be subtracted from the detector-response change to quantify a secondary contribution. A finite-size test further showed that oblique protons could traverse an edge-clipped path in a nominally thick shield. Within the discrete candidate set, 25 mm PE was the lowest-mass configuration with positive mean response reduction in all four benchmark fields. These results define transport and geometry regimes that should be checked before a shielding design is advanced to mission-specific modelling or experimental qualification.

Authors

Institutions

Publication Details

Journal
Eurasian journal of physics and functional materials
Published
2026-11-26
DOI
https://doi.org/10.32523/ejpfm.2026100405
Primary Topic
Particle Detector Development and Performance
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Detector-Level Transport Regimes inPolyethylene/Aluminium Shieldingof Silicon Sensors under Photon,Electron, and Proton Irradiation

Y. Havvat
Eurasian journal of physics and functional materials
Particle Detector Development and Performance
article

Detector-Level Transport Regimes inPolyethylene/Aluminium Shieldingof Silicon Sensors under Photon,Electron, and Proton Irradiation

Y. Havvat
article en

Abstract

Shielding performance inferred from attenuation or nominal thickness can misrepresent the response of a finite semiconductor detector. This study uses Geant4 to map energy deposited in a silicon sensor of dimensions 20 mm × 20 mm × 0.5 mm behind polyethylene (PE) and PE–aluminium (PE–Al) shields under controlled photon, electron, and proton fields. Event-level scoring separates primary survival, residual entry energy, shield-generated secondaries, and finite shield coverage. The proton response was strongly non-monotonic near range-out: effective suppression occurred between 8–9 mm PE at 30 MeV and between 20–25 mm PE at 50 MeV, in agreement with NIST PSTAR projected ranges. For photons, short shield-to-sensor gaps increased silicon energy deposition, consistent with enhanced acceptance of shield-generated secondaries. At the final 100 mm gap, adding 0.5 mm Al to 25 mm PE improved the photon-response reduction by 3.083 ± 0.558 percentage points under the reference physics list; the uncertainty is a two-sided 95% sampling confidence-interval half-width and excludes physics-model uncertainty. An XCOM narrow-beam calculation gave 1.01 percentage points of additional uncollided primary-photon number removal, a different observable that cannot be subtracted from the detector-response change to quantify a secondary contribution. A finite-size test further showed that oblique protons could traverse an edge-clipped path in a nominally thick shield. Within the discrete candidate set, 25 mm PE was the lowest-mass configuration with positive mean response reduction in all four benchmark fields. These results define transport and geometry regimes that should be checked before a shielding design is advanced to mission-specific modelling or experimental qualification.

Eurasian journal of physics and functional materialsVol. 10(04)
Cukurova University (TR)
Particle Detector Development and Performance
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon