Behavior of Concrete One-Way Slab Reinforced by GFRP Bars with a Novel Method of Reinforcement Splices
Fibre-reinforced polymers (FRP) have become a viable alternative to conventional steel reinforcement in concrete structures exposed to severe environmental conditions, owing to their high corrosion resistance and favorable mechanical properties. This study experimentally investigates the flexural behaviour of one-way concrete slabs reinforced with glass fibre-reinforced polymer (GFRP) bars and evaluates the effectiveness of a novel method for splicing GFRP reinforcement. The experimental program consisted of seven simply supported one-way concrete slabs with dimensions of 1000 × 400 × 70 mm, reinforced with 10 mm-diameter GFRP bars. The specimens were subjected to two-point loading until failure, with different reinforcement splice configurations adopted to investigate their influence on structural performance. The experimental variables included the splice configuration and its effect on the flexural response of the slabs. The measured parameters included cracking load, deflection at cracking and ultimate loads, ultimate load-carrying capacity, stiffness, ductility, toughness, and failure mode. The experimental results were evaluated in terms of the influence of the proposed splice method on the development of flexural strength and overall structural performance. The results were also compared with the predictions and design requirements of the ACI 440. Particular attention was given to the serviceability and ultimate limit states, considering the relatively low elastic modulus and different failure characteristics of GFRP reinforcement compared with conventional steel reinforcement. The findings demonstrate the effectiveness of the proposed splice technique and provide insight into its ability to develop adequate structural performance in GFRP-reinforced concrete slabs. The study indicates that an appropriately designed new splice can provide a practical solution for reinforcement continuity while maintaining satisfactory flexural strength, stiffness, and serviceability. The outcomes contribute to the development of more reliable design and detailing practices for GFRP-reinforced one-way concrete slabs, particularly where conventional steel reinforcement is unsuitable because of severe environmental exposure.
Authors
- Ziadoon Mohsin Ali (ORCID: https://orcid.org/0000-0002-8114-0990)
- Aleaa Basheer Radi (ORCID: https://orcid.org/0000-0002-6919-6588)
- Akram Shakir Mahmoud (ORCID: https://orcid.org/0000-0002-1956-0281)
- Aymen Hameed Fayyadh (ORCID: https://orcid.org/0009-0004-8814-9738)
- Omar Z. Amer (ORCID: https://orcid.org/0000-0001-8844-6071)
- Taghreed Kh. Mohammed
Institutions
- University of Anbar (IQ)
- Koya University (IQ)
Publication Details
- Journal
- Research Square
- Published
- 2026-11-26
- DOI
- https://doi.org/10.21203/rs.3.rs-11661402/v1
- Primary Topic
- Structural Behavior of Reinforced Concrete
- Type
- preprint