Precursor Chemistry Decides Phase Purity in Sol-Gel TiO2, ZnO and α-Fe2O3: Chloride- Urea Routes Retain Ammine and Ammonium Chloride By-Products
Sol-gel comparisons of oxide nanoparticles usually assume that identical processing gives equally clean products. We tested this for TiO2, ZnO and α-Fe2O3 prepared with fixed precursor concentration, aging, drying and calcination (400-500 °C, 2 h), changing only the precursor-solvent pair. The titanium isopropoxide-acetic acid route gave phase-pure anatase (6.9 nm crystallites) whose only residue was surface acetate. The ZnCl2-urea and FeCl3-urea routes did not give clean oxides. Their XRD patterns are dominated by reflections foreign to wurtzite and hematite, their FTIR spectra show N-H and NH3/NH4+ deformation bands, and EDX finds 59.7 and 23.4 at.% Cl. Read together, these signatures point to diamminedichlorozinc, Zn(NH3)2Cl2, in the zinc product and ammonium chloride in the iron product. The by-products also track morphology: fused microplates for zinc, loosely clustered nanograins for iron, and fractured flakes for titanium. Since neither phase should survive 400 °C, they likely re-formed on cooling or escaped decomposition in the powder bed. Chloride-urea sol-gel products therefore need explicit phase verification before oxide properties are attributed to them.
Authors
- I. B. Patel (ORCID: https://orcid.org/0000-0002-6021-6968)
- Khyati Mody
Institutions
- Veer Narmad South Gujarat University (IN)
Publication Details
- Journal
- International Journal of Science and Research (IJSR)
- Published
- 2026-11-26
- DOI
- https://doi.org/10.21275/sr261124095404
- Primary Topic
- Chemical and Physical Properties of Materials
- Type
- article
- Field-Weighted Citation Impact
- 0.00