Mechanical property enhancement of laser powder bed fusion additive manufacturing – AlSi10Mg parts with aging and hot isostatic pressing processes: Mechanical considerations

In this work, the influence of post-treatment on the physical and mechanical properties of AlSi10Mg processed by laser powder bed fusion (L-PBF) on an EOS M 290 machine in three build orientations (0°, 45° and 90°) was analyzed quantitatively. The post-treatments comprised solution treatment (530 °C/2 h, water quenching) followed by natural aging (T4 temper) or by artificial aging at 150, 175 or 200 °C for 2 h (T6 temper), as well as hot isostatic pressing (HIP; 530 °C, 100 MPa, 2 h) and HIP followed by T6 aging at 175 °C (HIP + T6). Density measurements, Vickers hardness (HV0.2) tests, tensile tests, impulse excitation measurements of Young's modulus and fractography were carried out. The as-fabricated (AF) state showed the highest strength (ultimate tensile strength 474–506 MPa, yield strength 237–287 MPa) but the lowest elongation (≈6–10%) and a relative density of 97.6–98.9%. Solution treatment and aging decreased the strength by 35–40% and increased the elongation to ≈12–22%, but did not affect the porosity; aging at 175 °C gave the best T6 properties. HIP increased the relative density to 99.1–99.7% but halved the hardness, whereas HIP + T6 combined a relative density of 99.8–99.96% with ≈75–90% of the AF hardness, a tensile strength of ≈295–325 MPa and an elongation of ≈10–12.5%, and reduced the orientation-related difference in density from 1.24 to 0.14 percentage points. The findings of this comprehensive parametric study indicate that HIP + T6 provides the optimal combination of properties for meeting the mechanical requirements of industrial applications.

Authors

Institutions

Publication Details

Journal
Proceedings of the Institution of Mechanical Engineers Part L Journal of Materials Design and Applications
Published
2026-11-26
DOI
https://doi.org/10.1177/14644207261511127
Primary Topic
Additive Manufacturing Materials and Processes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Mechanical property enhancement of laser powder bed fusion additive manufacturing – AlSi10Mg parts with aging and hot isostatic pressing processes: Mechanical considerations

Remzi Ecmel Ece, Ömer Keleş, Bekir Sami Yilbaş
Proceedings of the Institution of Mechanical Engineers Part L Journal of Materials Design and Applications
Additive Manufacturing Materials and Processes
article

Mechanical property enhancement of laser powder bed fusion additive manufacturing – AlSi10Mg parts with aging and hot isostatic pressing processes: Mechanical considerations

Remzi Ecmel Ece, Ömer Keleş, Bekir Sami Yilbaş
article en

Abstract

In this work, the influence of post-treatment on the physical and mechanical properties of AlSi10Mg processed by laser powder bed fusion (L-PBF) on an EOS M 290 machine in three build orientations (0°, 45° and 90°) was analyzed quantitatively. The post-treatments comprised solution treatment (530 °C/2 h, water quenching) followed by natural aging (T4 temper) or by artificial aging at 150, 175 or 200 °C for 2 h (T6 temper), as well as hot isostatic pressing (HIP; 530 °C, 100 MPa, 2 h) and HIP followed by T6 aging at 175 °C (HIP + T6). Density measurements, Vickers hardness (HV0.2) tests, tensile tests, impulse excitation measurements of Young's modulus and fractography were carried out. The as-fabricated (AF) state showed the highest strength (ultimate tensile strength 474–506 MPa, yield strength 237–287 MPa) but the lowest elongation (≈6–10%) and a relative density of 97.6–98.9%. Solution treatment and aging decreased the strength by 35–40% and increased the elongation to ≈12–22%, but did not affect the porosity; aging at 175 °C gave the best T6 properties. HIP increased the relative density to 99.1–99.7% but halved the hardness, whereas HIP + T6 combined a relative density of 99.8–99.96% with ≈75–90% of the AF hardness, a tensile strength of ≈295–325 MPa and an elongation of ≈10–12.5%, and reduced the orientation-related difference in density from 1.24 to 0.14 percentage points. The findings of this comprehensive parametric study indicate that HIP + T6 provides the optimal combination of properties for meeting the mechanical requirements of industrial applications.

Proceedings of the Institution of Mechanical Engineers Part L Journal of Materials Design and Applications
King Fahd University of Petroleum and Minerals (SA), Turkish Aerospace Industries (Turkey) (TR), Gazi University (TR)
Additive Manufacturing Materials and Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon