Improving Welding Efficiency and Mechanical Performance in Industrial Applications: A Study of Filler Metal Welds Using GTAW
This research investigated the Gas Tungsten Arc Welding (GTAW) process for dissimilar metal joints between A335 P11 and A312 TP304 pipes, which are commonly used in industrial applications such as water-tube boilers. The study focused on improving process efficiency, weld quality, and mechanical performance using pipes with an outside diameter of 89 mm, a length of 130 mm, and a wall thickness of 5.54 mm. Welding was performed using Ni625/ER NiCrMo-3 filler metal and a RILON TIG 200S welding machine. The optimized welding parameters consisted of a welding current of 120 A, a welding speed of 13.7 mm/min, and a shielding gas flow rate of 16 L/min. Mechanical and metallurgical evaluations demonstrated a maximum tensile strength of 675 MPa and a hardness of 230.4 HV. The impact test revealed that the Heat-Affected Zone (HAZ) of A312 TP304 exhibited greater toughness than that of A335 P11. Bend tests confirmed the structural integrity of the welded joints, with no cracks observed after 180° bending. These findings highlight the potential of the GTAW process as an efficient and reliable method for dissimilar metal welding in industrial manufacturing, contributing to improved production efficiency and reduced defect rates in critical applications.
Authors
- Bundit Inseemeesak
- Yodnapha Ketmuang (ORCID: https://orcid.org/0009-0009-1146-6360)
- Bundit Wongthong
Publication Details
- Journal
- The Journal of King Mongkut s University of Technology North Bangkok
- Published
- 2026-11-26
- DOI
- https://doi.org/10.14416/j.kmutnb.2026.11.005
- Primary Topic
- Welding Techniques and Residual Stresses
- Type
- article
- Field-Weighted Citation Impact
- 0.00