Hot cracking in high strength carbon steel weld joints
In the present study, the hot cracking susceptibility of the submerged arc weld metal in steel plates for the shipbuilding and wind tower industries was investigated. The susceptibility was predominantly determined by the chemical composition of the fusion zone, particularly the carbon, phosphorus, and sulfur contents. The weld metal composition was governed by the wire and flux compositions, flux basicity, and the extent of base metal dilution. Transverse Varestraint tests were performed to quantitatively analyze the cracking behavior, determine the weld metal compositions required to prevent hot cracking, and identify the optimum welding consumables for each steel grade. The effects of alloying elements and impurity contents on hot cracking susceptibility were investigated by comparing the brittle temperature range (BTR) obtained from the Varestraint tests with thermodynamic calculations of solidification behavior as a function of weld metal composition.
Authors
- Younghwan Park
- Kyutae Han (ORCID: https://orcid.org/0000-0002-9561-2004)
- Seunggab Hong
Institutions
- Pohang Iron and Steel (South Korea) (KR)
Publication Details
- Journal
- Research Square
- Published
- 2026-11-26
- DOI
- https://doi.org/10.21203/rs.3.rs-11599535/v1
- Primary Topic
- Welding Techniques and Residual Stresses
- Type
- preprint