Flow-enhanced MgSO4 attack on alkali-activated slag concrete: sulfate ingress, alkalinity loss and microstructural evolution

To investigate sulfate ingress, pore solution alkalinity loss, and microstructural evolution of alkali-activated slag concrete (AASC) under flowing MgSO 4 exposure, static (0 m/s) and flowing (0.5 m/s) conditions were established using a 5% MgSO 4 solution, with exposure periods ranging from 15 to 180 days. Free and total sulfate contents were measured at different depths. The depth-weighted mean sulfate content and flow enhancement factor were further used to quantify the effect of solution flow on sulfate ingress. X-ray diffraction, scanning electron microscopy, low-field nuclear magnetic resonance, and pH measurements were also conducted to characterize phase composition, micromorphology, pore structure, and pore solution alkalinity. Both free and total sulfate contents increased with exposure time and decreased with increasing depth from the exposed surface. The 0.5 m/s flowing condition markedly increased the overall sulfate ingress. At 15 days, the flow enhancement factors for free and total sulfate reached 70.8% and 68.3%, respectively, and then gradually decreased to about 30% at 180 days. As exposure progressed, pore solution alkalinity continuously decreased, the diffraction features associated with C-A-S-H gradually weakened, while those of gypsum, ettringite, and Mg-bearing reaction products became more pronounced. Under long-term exposure, solution flow further promoted matrix loosening, microcrack development, and pore coarsening. At 180 days, the total porosity increased from 8.4% under static conditions to 11.9% under flowing conditions, while the proportion of pores larger than 50 nm increased from 47.6% to 71.4%. Overall, solution flow accelerated sulfate transport and pore solution alkalinity loss, thereby promoting binder-phase degradation and pore coarsening and intensifying the long-term deterioration of AASC under MgSO 4 exposure.

Authors

Institutions

Publication Details

Journal
Frontiers in Materials
Published
2026-11-26
DOI
https://doi.org/10.3389/fmats.2026.2017210
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Flow-enhanced MgSO4 attack on alkali-activated slag concrete: sulfate ingress, alkalinity loss and microstructural evolution

Shaofeng Zhang, Changqi Tian
Frontiers in Materials
Concrete and Cement Materials Research
article

Flow-enhanced MgSO4 attack on alkali-activated slag concrete: sulfate ingress, alkalinity loss and microstructural evolution

Shaofeng Zhang, Changqi Tian
article en

Abstract

To investigate sulfate ingress, pore solution alkalinity loss, and microstructural evolution of alkali-activated slag concrete (AASC) under flowing MgSO 4 exposure, static (0 m/s) and flowing (0.5 m/s) conditions were established using a 5% MgSO 4 solution, with exposure periods ranging from 15 to 180 days. Free and total sulfate contents were measured at different depths. The depth-weighted mean sulfate content and flow enhancement factor were further used to quantify the effect of solution flow on sulfate ingress. X-ray diffraction, scanning electron microscopy, low-field nuclear magnetic resonance, and pH measurements were also conducted to characterize phase composition, micromorphology, pore structure, and pore solution alkalinity. Both free and total sulfate contents increased with exposure time and decreased with increasing depth from the exposed surface. The 0.5 m/s flowing condition markedly increased the overall sulfate ingress. At 15 days, the flow enhancement factors for free and total sulfate reached 70.8% and 68.3%, respectively, and then gradually decreased to about 30% at 180 days. As exposure progressed, pore solution alkalinity continuously decreased, the diffraction features associated with C-A-S-H gradually weakened, while those of gypsum, ettringite, and Mg-bearing reaction products became more pronounced. Under long-term exposure, solution flow further promoted matrix loosening, microcrack development, and pore coarsening. At 180 days, the total porosity increased from 8.4% under static conditions to 11.9% under flowing conditions, while the proportion of pores larger than 50 nm increased from 47.6% to 71.4%. Overall, solution flow accelerated sulfate transport and pore solution alkalinity loss, thereby promoting binder-phase degradation and pore coarsening and intensifying the long-term deterioration of AASC under MgSO 4 exposure.

Frontiers in MaterialsVol. 13
Shaanxi Railway Institute (CN)
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
Flow-enhanced MgSO4 attack on alkali-activated slag concrete: sulfate ingress, alkalinity loss and microstructural evolution — Shaofeng Zhang, Changqi Tian · Frontiers in Materials (2026) | TGRS Research Map | TGRS