Distinguishing Symptoms From Etiology: A Cascading Degradation Mechanism in Cobalt‐Free Layered Cathodes

Cobalt‐free layered cathodes are pivotal for next‐generation lithium‐ion batteries due to their cost‐effectiveness, high energy density, and sustainability. However, the complex interplay between severe structural disorder and intrinsic degradation factors remains elusive, hindering their rational design and practical application. Herein, this study reveals a “cascading degradation mechanism” that decouples initial disorder from dynamic deterioration, identifying intrinsic oxygen vacancies as the fundamental “etiology” while distinguishing accumulated cation disorder as a “symptom.” Leveraging multi‐scale characterization on model LiNi 0.6 Mn 0.4 O 2 and Density Functional Theory calculations, the results demonstrate that intrinsic oxygen vacancies trigger a triple synergistic effect of aggravated lattice distortion, high‐voltage oxygen loss, and accelerated interfacial side reactions, which kinetically facilitates Ni migration, driving irreversible structural degradation. Consequently, this work establishes the Li/Ni disorder accumulation (ΔLi/Ni) in limited cycles as a dynamic indicator for evaluating long‐term stability. Based on this mechanism, the optimized NM‐880 cathode delivers excellent long‐term stability, achieving a 92.37% capacity retention after 400 cycles at 0.5 C. The universality of this indicator is robustly validated in commercial LiNi 0.6 Co 0.2 Mn 0.2 O 2 and LiNi 0.5 Co 0.2 Mn 0.3 O 2 systems. This work signals a paradigm shift in cathode design: moving from optimizing static initial structures to regulating defect‐induced dynamic evolution.

Authors

Institutions

Publication Details

Journal
Advanced Functional Materials
Published
2026-11-26
DOI
https://doi.org/10.1002/adfm.79697
Primary Topic
Lithium- and Sodium-Ion Battery Electrodes
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Distinguishing Symptoms From Etiology: A Cascading Degradation Mechanism in Cobalt‐Free Layered Cathodes

Hongtao Sun, Haitao Huang, Bingan Lu, Fangrui Yu et al.
Advanced Functional Materials
Lithium- and Sodium-Ion Battery Electrodes
article

Distinguishing Symptoms From Etiology: A Cascading Degradation Mechanism in Cobalt‐Free Layered Cathodes

Hongtao Sun, Haitao Huang, Bingan Lu, Fangrui Yu, Jian Zhu, Cheng Chao Li, Zhiqun Zhou, 云亮, Jingyao YANG, Yuanyuan Li, Hongli Deng, Qiusheng Zhang, Ye Zhang
article en

Abstract

Cobalt‐free layered cathodes are pivotal for next‐generation lithium‐ion batteries due to their cost‐effectiveness, high energy density, and sustainability. However, the complex interplay between severe structural disorder and intrinsic degradation factors remains elusive, hindering their rational design and practical application. Herein, this study reveals a “cascading degradation mechanism” that decouples initial disorder from dynamic deterioration, identifying intrinsic oxygen vacancies as the fundamental “etiology” while distinguishing accumulated cation disorder as a “symptom.” Leveraging multi‐scale characterization on model LiNi 0.6 Mn 0.4 O 2 and Density Functional Theory calculations, the results demonstrate that intrinsic oxygen vacancies trigger a triple synergistic effect of aggravated lattice distortion, high‐voltage oxygen loss, and accelerated interfacial side reactions, which kinetically facilitates Ni migration, driving irreversible structural degradation. Consequently, this work establishes the Li/Ni disorder accumulation (ΔLi/Ni) in limited cycles as a dynamic indicator for evaluating long‐term stability. Based on this mechanism, the optimized NM‐880 cathode delivers excellent long‐term stability, achieving a 92.37% capacity retention after 400 cycles at 0.5 C. The universality of this indicator is robustly validated in commercial LiNi 0.6 Co 0.2 Mn 0.2 O 2 and LiNi 0.5 Co 0.2 Mn 0.3 O 2 systems. This work signals a paradigm shift in cathode design: moving from optimizing static initial structures to regulating defect‐induced dynamic evolution.

Advanced Functional Materials
Pennsylvania State University (US), Guangdong University of Technology (CN), Hunan University (CN), Contemporary Amperex Technology Co., Limited. (CN)
Lithium- and Sodium-Ion Battery Electrodes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon