Effects of Cerium and Boron Precursor Loading on the Structural, Morphological and Raman Properties of Sol–Gel-Derived Ce/B Co-Doped Tio₂

Pure TiO₂ and four Ce/B co-doped TiO₂ powders were prepared by a single modified sol–gel route in which cerium(III) nitrate and boric acid were added together to the same titanium sol (simultaneous co-doping, not separate single-dopant series). The loading parameter is the nominal elemental content of each dopant relative to the theoretical TiO₂ yield; both dopants were increased together, giving 1.5 wt% Ce + 2 wt% B (Ce1.5B2), 1.8 wt% Ce + 3 wt% B (Ce1.8B3), 2.1 wt% Ce + 4 wt% B (Ce2.1B4) and 2.4 wt% Ce + 5 wt% B (Ce2.4B5), i.e. a total nominal loading of 3.5–7.4 wt% (Ce/Ti ≈ 0.9–1.4 at%, B/Ti ≈ 15–37 at%). Tetrabutyl titanate and titanium(III) chloride were the titanium sources, and all gels were dried at 100 °C and calcined at 500 °C for 5 h in air. The effect of precursor loading on crystallinity, phase composition, lattice parameters, agglomerate morphology and vibrational properties was examined by X-ray diffraction (XRD) with Scherrer, Williamson–Hall and lattice-parameter analysis, scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDX) and Raman spectroscopy, supported by FTIR and UV–Vis measurements. All samples were anatase-dominant, with a minor brookite component and no detectable rutile or crystalline CeO₂. The Scherrer crystallite size decreased from 11.8 nm (pure TiO₂) to 6.3, 6.5, 5.9 and 5.5 nm with increasing loading; most of the reduction occurred at the lowest loading. The a parameter was unchanged (3.786–3.789 Å) and c was slightly lower in the doped samples (9.479–9.490 Å versus 9.506 Å), a difference close to the fitting uncertainty. SEM showed dense micrometre-scale agglomerates for Ce1.5B2–Ce2.1B4 and finer, more dispersed agglomerates for Ce2.4B5. EDX detected Ce in all doped samples with large spot-to-spot variation (1.10–9.82 wt%); boron could not be quantified by EDX. The Raman Eg(3) band broadened from 28.3 to 41.6–48.1 cm⁻¹, increasing with loading, consistent with smaller crystallites and greater lattice disorder. The highest loading (Ce2.4B5) gave the smallest crystallites and the broadest Raman band. These loading-dependent structural data provide a basis for modified TiO₂ intended for photocatalytic and optical applications; boron incorporation, dopant location and functional performance remain to be established.

Authors

Institutions

Publication Details

Journal
International Journal of Latest Technology in Engineering Management & Applied Science
Published
2026-11-26
DOI
https://doi.org/10.51583/ijltemas.2026.151100053
Primary Topic
TiO2 Photocatalysis and Solar Cells
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effects of Cerium and Boron Precursor Loading on the Structural, Morphological and Raman Properties of Sol–Gel-Derived Ce/B Co-Doped Tio₂

C. V. Krishna Reddy, K. Jhansirani
International Journal of Latest Technology in Engineering Management & Applied Science
TiO2 Photocatalysis and Solar Cells
article

Effects of Cerium and Boron Precursor Loading on the Structural, Morphological and Raman Properties of Sol–Gel-Derived Ce/B Co-Doped Tio₂

C. V. Krishna Reddy, K. Jhansirani
article en

Abstract

Pure TiO₂ and four Ce/B co-doped TiO₂ powders were prepared by a single modified sol–gel route in which cerium(III) nitrate and boric acid were added together to the same titanium sol (simultaneous co-doping, not separate single-dopant series). The loading parameter is the nominal elemental content of each dopant relative to the theoretical TiO₂ yield; both dopants were increased together, giving 1.5 wt% Ce + 2 wt% B (Ce1.5B2), 1.8 wt% Ce + 3 wt% B (Ce1.8B3), 2.1 wt% Ce + 4 wt% B (Ce2.1B4) and 2.4 wt% Ce + 5 wt% B (Ce2.4B5), i.e. a total nominal loading of 3.5–7.4 wt% (Ce/Ti ≈ 0.9–1.4 at%, B/Ti ≈ 15–37 at%). Tetrabutyl titanate and titanium(III) chloride were the titanium sources, and all gels were dried at 100 °C and calcined at 500 °C for 5 h in air. The effect of precursor loading on crystallinity, phase composition, lattice parameters, agglomerate morphology and vibrational properties was examined by X-ray diffraction (XRD) with Scherrer, Williamson–Hall and lattice-parameter analysis, scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDX) and Raman spectroscopy, supported by FTIR and UV–Vis measurements. All samples were anatase-dominant, with a minor brookite component and no detectable rutile or crystalline CeO₂. The Scherrer crystallite size decreased from 11.8 nm (pure TiO₂) to 6.3, 6.5, 5.9 and 5.5 nm with increasing loading; most of the reduction occurred at the lowest loading. The a parameter was unchanged (3.786–3.789 Å) and c was slightly lower in the doped samples (9.479–9.490 Å versus 9.506 Å), a difference close to the fitting uncertainty. SEM showed dense micrometre-scale agglomerates for Ce1.5B2–Ce2.1B4 and finer, more dispersed agglomerates for Ce2.4B5. EDX detected Ce in all doped samples with large spot-to-spot variation (1.10–9.82 wt%); boron could not be quantified by EDX. The Raman Eg(3) band broadened from 28.3 to 41.6–48.1 cm⁻¹, increasing with loading, consistent with smaller crystallites and greater lattice disorder. The highest loading (Ce2.4B5) gave the smallest crystallites and the broadest Raman band. These loading-dependent structural data provide a basis for modified TiO₂ intended for photocatalytic and optical applications; boron incorporation, dopant location and functional performance remain to be established.

International Journal of Latest Technology in Engineering Management & Applied ScienceVol. 15(11)
Rayalaseema University (IN)
TiO2 Photocatalysis and Solar Cells
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon