Nanochaperone-mediated dynamic protection of protein conformation enables sustained enzymatic degradation of highly crystalline polylactic acid
. By combining alkaline pretreatment with a cyclic "work-rest" heating protocol, highly crystalline PLLA and post-consumer PLA were degraded at 70 °C, achieving >85% degradation within five days with high-purity lactic acid recovery. This work establishes dynamic conformational protection as a new design principle for high-temperature biocatalysis and enzymatic polyester upcycling.
Authors
- Feihe Ma (ORCID: https://orcid.org/0000-0002-8511-3922)
- Chen Shijia
- Linqi Shi
- Wenyi Gui
- Hongyun Liu
Institutions
- Nankai University (CN)
- State Key Laboratory of Medicinal Chemical Biology (CN)
Publication Details
- Journal
- Materials Horizons
- Published
- 2026-11-26
- DOI
- https://doi.org/10.1039/d6mh01570k
- Primary Topic
- biodegradable polymer synthesis and properties
- Type
- article
- Field-Weighted Citation Impact
- 0.00