Effects of Sulfoaluminate Cement Content and Anti-Washout Admixture Dosage on the Performance and Hydration Behavior of Underwater Concrete

Although cementitious materials and anti-washout admixtures have each been investigated in underwater concrete, the combined effects remain insufficiently understood, and the trade-off between washout resistance and workability that governs the usable dosage range remains insufficiently quantified. How sulfoaluminate cement (SAC) content and the dosage of UWB-II, a polysaccharide-based anti-washout admixture, jointly affect the washout resistance, workability, mechanical properties, hydration behavior, and microstructure of underwater concrete under different casting conditions was examined. The SAC (6% and 8%) and anti-washout admixture (UWB-II, 0%, 0.5%, 1.0%, 1.5%, 2.0%, and 2.5%) was added. The evaluation combined net concrete mass loss, suspended solids content, pH, flowability, setting time, and compressive strength tests with isothermal calorimetry, XRD, TG-DTG, MIP, and SEM analyses. The results showed that increasing the UWB-II dosage improved washout resistance of anti-washout underwater concrete, with net concrete mass loss recorded as 0% (below the detection limit) at a dosage of 2.0%. However, higher UWB-II dosages reduced flowability and prolonged both initial and final setting times, as measured directly on fresh pastes, whereas isothermal calorimetry of cement pastes independently showed a delayed main exothermic peak, consistent with the setting time results. At a given UWB-II dosage, the 8% SAC system showed lower net concrete mass loss and shorter setting times than the 6% SAC system: without UWB-II, the net concrete mass loss was 18.0% and 13.3% for the S6 and S8 systems, respectively, and at 1.5% UWB-II, increasing the SAC content from 6% to 8% shortened the initial and final setting times by 344 min and 180 min. Underwater compressive strength initially increased and then decreased with increasing UWB-II dosage. The mixture containing 8% SAC and 1.5% UWB-II achieved the highest 7 d underwater compressive strength of 37.3 MPa, representing a 40.8% increase compared with the mixture without UWB-II. SAC content, UWB-II dosage, and casting conditions affected hydration product characteristics and pore structure without substantially altering the major crystalline phases. Under the tested conditions, a UWB-II dosage of 2.0% reduced the recorded net concrete mass loss to zero in both SAC systems, whereas the highest 7 d underwater compressive strength was achieved with 8% SAC and 1.5% UWB-II, highlighting the trade-offs among washout resistance, flowability, setting time, and compressive strength within the investigated mixture range.

Authors

Institutions

Publication Details

Journal
Materials
Published
2026-11-26
DOI
https://doi.org/10.3390/ma19235026
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effects of Sulfoaluminate Cement Content and Anti-Washout Admixture Dosage on the Performance and Hydration Behavior of Underwater Concrete

Xiaodong Ma, Runzhuo Cao, Yichao Hao, Xihe Zhang et al.
Materials
Concrete and Cement Materials Research
article

Effects of Sulfoaluminate Cement Content and Anti-Washout Admixture Dosage on the Performance and Hydration Behavior of Underwater Concrete

Xiaodong Ma, Runzhuo Cao, Yichao Hao, Xihe Zhang, Jialong Guo, Jinglong Zhao
article en

Abstract

Although cementitious materials and anti-washout admixtures have each been investigated in underwater concrete, the combined effects remain insufficiently understood, and the trade-off between washout resistance and workability that governs the usable dosage range remains insufficiently quantified. How sulfoaluminate cement (SAC) content and the dosage of UWB-II, a polysaccharide-based anti-washout admixture, jointly affect the washout resistance, workability, mechanical properties, hydration behavior, and microstructure of underwater concrete under different casting conditions was examined. The SAC (6% and 8%) and anti-washout admixture (UWB-II, 0%, 0.5%, 1.0%, 1.5%, 2.0%, and 2.5%) was added. The evaluation combined net concrete mass loss, suspended solids content, pH, flowability, setting time, and compressive strength tests with isothermal calorimetry, XRD, TG-DTG, MIP, and SEM analyses. The results showed that increasing the UWB-II dosage improved washout resistance of anti-washout underwater concrete, with net concrete mass loss recorded as 0% (below the detection limit) at a dosage of 2.0%. However, higher UWB-II dosages reduced flowability and prolonged both initial and final setting times, as measured directly on fresh pastes, whereas isothermal calorimetry of cement pastes independently showed a delayed main exothermic peak, consistent with the setting time results. At a given UWB-II dosage, the 8% SAC system showed lower net concrete mass loss and shorter setting times than the 6% SAC system: without UWB-II, the net concrete mass loss was 18.0% and 13.3% for the S6 and S8 systems, respectively, and at 1.5% UWB-II, increasing the SAC content from 6% to 8% shortened the initial and final setting times by 344 min and 180 min. Underwater compressive strength initially increased and then decreased with increasing UWB-II dosage. The mixture containing 8% SAC and 1.5% UWB-II achieved the highest 7 d underwater compressive strength of 37.3 MPa, representing a 40.8% increase compared with the mixture without UWB-II. SAC content, UWB-II dosage, and casting conditions affected hydration product characteristics and pore structure without substantially altering the major crystalline phases. Under the tested conditions, a UWB-II dosage of 2.0% reduced the recorded net concrete mass loss to zero in both SAC systems, whereas the highest 7 d underwater compressive strength was achieved with 8% SAC and 1.5% UWB-II, highlighting the trade-offs among washout resistance, flowability, setting time, and compressive strength within the investigated mixture range.

MaterialsVol. 19(23)
Xi'an University of Architecture and Technology (CN), Shandong University (CN), Shanxi University (CN), PowerChina (China) (CN)
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon