Fretting wear of laser textured Ti-6Al-4 V against Si₃N₄ under varied groove orientation and spacing
Ti-6Al-4 V titanium alloy widely used in aerospace components suffers severe fretting damage at blade-disc interfaces, prompting the development of laser surface texturing (LST) to mitigate wear. While prior studies have established texture efficacy in homologous contacts, the tribological behavior of textured titanium against hard ceramic counter-bodies remains poorly understood. This study systematically investigated the fretting performance of laser-textured Ti-6Al-4 V against Si₃N₄ ceramic, examining three groove orientations (perpendicular, parallel, and 45° oblique to sliding) and two spacings (80 μm and 120 μm) under normal loads of 20–100 N. Perpendicular grooves (80 μm) achieved the lowest coefficient of friction and system deformation by segmenting the contact area and impeding shear stress transmission, yet underwent severe plastic collapse at 100 N due to buckling of thin inter-groove ridges. In contrast, parallel-oriented grooves and wider spacing (120 μm) maintained structural integrity under extreme loads with minimal indentation, albeit at slightly higher friction. These results demonstrate that in hard/soft fretting contacts, surface texture functions primarily as a modulator of contact mechanics rather than debris management, revealing a critical design trade-off between friction reduction and load-bearing capacity that must guide texture optimization for aerospace applications.
Authors
- Yueyang Xia (ORCID: https://orcid.org/0000-0003-0964-4876)
- Jianfei Wang (ORCID: https://orcid.org/0000-0001-8681-7465)
- Xiaoming Yang
- Shihao Mao
- Changzi Chen
- Bo Zhao
- Liang Chai
Institutions
- Jingchu University of Technology (CN)
Publication Details
- Journal
- Scientific Reports
- Published
- 2026-11-26
- DOI
- https://doi.org/10.1038/s41598-026-81593-9
- Primary Topic
- Mechanical stress and fatigue analysis
- Type
- article
- Field-Weighted Citation Impact
- 0.00