Cyanide-Free Pyrophosphate Electrodeposition of a Ni-P-W/Ni Bilayer Coating for Wear and Corrosion Protection of X70 Steel

Wear and corrosion often coexist in petroleum service environments, yet single-function coatings rarely provide durable combined protection. Here, a Ni-P-W/Ni bilayer coating was fabricated on X70 pipeline steel by direct-current electrodeposition from a cyanide-free pyrophosphate bath, followed by annealing at 700 °C for 2 h. The coating consisted of an approximately 30.7 μm thick Ni-P-W outer layer and a 41.5 μm thick Ni inner layer. Both interfaces were continuous, and P and W were confined to the outer layer. Under dry ball-on-disk sliding, the specific wear rate was approximately 8.5 × 10−7 mm3/(N·m), and the maximum wear depth remained within 16–20% of the outer-layer thickness. In 3.5 wt.% NaCl solution, the coating shifted Ecorr from −0.64 to −0.41 VSCE and reduced icorr from 8.82 × 10−5 to 9.08 × 10−7 A/cm2, with a passive region up to Eb = −0.11 VSCE. EIS revealed high film and charge-transfer resistances. The Ni underlayer and Ni-P-W outer layer provide a feasible electrodeposition strategy for combined wear and corrosion protection of pipeline steel.

Authors

Institutions

Publication Details

Journal
Materials
Published
2026-11-26
DOI
https://doi.org/10.3390/ma19235034
Primary Topic
Electrodeposition and Electroless Coatings
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Cyanide-Free Pyrophosphate Electrodeposition of a Ni-P-W/Ni Bilayer Coating for Wear and Corrosion Protection of X70 Steel

Ying Yue, Zitong Niu, Siyu Gu, Jinpeng Liu et al.
Materials
Electrodeposition and Electroless Coatings
article

Cyanide-Free Pyrophosphate Electrodeposition of a Ni-P-W/Ni Bilayer Coating for Wear and Corrosion Protection of X70 Steel

Ying Yue, Zitong Niu, Siyu Gu, Jinpeng Liu, Xiaochen Zhang, Andong Wang
article en

Abstract

Wear and corrosion often coexist in petroleum service environments, yet single-function coatings rarely provide durable combined protection. Here, a Ni-P-W/Ni bilayer coating was fabricated on X70 pipeline steel by direct-current electrodeposition from a cyanide-free pyrophosphate bath, followed by annealing at 700 °C for 2 h. The coating consisted of an approximately 30.7 μm thick Ni-P-W outer layer and a 41.5 μm thick Ni inner layer. Both interfaces were continuous, and P and W were confined to the outer layer. Under dry ball-on-disk sliding, the specific wear rate was approximately 8.5 × 10−7 mm3/(N·m), and the maximum wear depth remained within 16–20% of the outer-layer thickness. In 3.5 wt.% NaCl solution, the coating shifted Ecorr from −0.64 to −0.41 VSCE and reduced icorr from 8.82 × 10−5 to 9.08 × 10−7 A/cm2, with a passive region up to Eb = −0.11 VSCE. EIS revealed high film and charge-transfer resistances. The Ni underlayer and Ni-P-W outer layer provide a feasible electrodeposition strategy for combined wear and corrosion protection of pipeline steel.

MaterialsVol. 19(23)
Shengli Oilfield Central Hospital (CN), Heilongjiang Institute of Technology (CN), Dongying Vocational Institute (CN), Shandong Institute of Petroleum and Chemical Technology (CN)
Electrodeposition and Electroless Coatings
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon