Effect of Tempering Temperature on the Wear Resistance of 9Cr18MoV Martensitic Bearing Steel
As a martensitic stainless steel, 9Cr18MoV steel is widely used in special bearing applications owing to its excellent wear and corrosion resistance. The effects of tempering temperature on the microstructure and mechanical properties of 9Cr18MoV steel were analyzed using optical microscopy (OM), Vickers hardness testing, X‐ray diffraction (XRD), scanning electron microscopy (SEM), and reciprocating friction and wear testing. The results show that as the tempering temperature increased from 160 to 200 °C, the retained austenite content decreased monotonically from 22.01% to 15.35%, while the volume fraction of carbides increased monotonically from 1.23% to 2.92%. This microstructural evolution led to a monotonic reduction in the hardness of the material from 711.22 HV 0.3 to 631.62 HV 0.3. However, the wear resistance first decreased and then increased, which was related to the combined effects of hardness and microstructure, particularly the reinforcement of the carbide skeleton. The optimal wear resistance was achieved at the tempering temperature of 160 °C.
Authors
- Yanbin Li
- Xingfu Yu (ORCID: https://orcid.org/0000-0002-8805-3275)
- Yong Su
- Lingyou Kong
- Yinghua Wei
- Yahua Hao
- Xiangxin Wang
- Jingui Xie
- Bo Li
Institutions
- Shenyang University of Technology (CN)
- Genertec Shenyang Machine Tool Co., Ltd. (China) (CN)
- Shenyang University of Chemical Technology (CN)
Publication Details
- Journal
- steel research international
- Published
- 2026-11-25
- DOI
- https://doi.org/10.1002/srin.70804
- Primary Topic
- Metal Alloys Wear and Properties
- Type
- article
- Field-Weighted Citation Impact
- 0.00