Experimental Investigation on Polypropylene Fiber-Reinforced Concrete with Partial Replacement of Cement by Quartz Powder
Ordinary Portland cement (OPC) is the primary binding agent in conventional concrete, but its industrial synthesisaccounts for significant energy consumption and carbon dioxide emissions. This investigation evaluates the performance of M30grade concrete produced by incorporating Quartz Powder (QP) as a partial replacement for OPC alongside Polypropylene Fiber(PPF) as secondary reinforcement. The research was carried out in two distinct experimental phases: Phase 1 identified the optimalreplacement fraction of QP (evaluated at 5%, 10%, 15%, and 20% by weight of cement), while Phase 2 investigated the synergisticaddition of PPF (at 0.5%, 1.0%, and 1.5% by volume) to the optimized QP matrix. Mechanical strength parameters includingcompressive strength across 3, 7, 28, and 56 days, 28-day split tensile strength, flexural strength, drop-weight impact resistance,and static modulus of elasticity were systematically assessed. Additionally, chemical durability was quantified through 28-dayimmersion tests in 5% HCl and 5% MgSO₄ solutions. Experimental results demonstrate that a 10% QP replacement level yieldsoptimal particle packing and hydration performance, achieving a 28-day compressive strength of 44.1 N/mm² (a 9.80% increaseover the control concrete), split tensile strength of 3.2 N/mm² (+12.98%), flexural strength of 4.7 N/mm² (+10.83%), and failureimpact energy of 753.1 J (37 blows). Incorporating 1.0% PPF into this 10% QP matrix further enhanced overall mechanicalperformance, achieving peak compressive strengths of 26.6, 33.0, 46.9, and 50.1 N/mm² at 3, 7, 28, and 56 days, respectively. At 28days, this hybrid mix achieved a split tensile strength of 4.6 N/mm² (+59.51% over control) and a flexural strength of 6.0 N/mm²(+40.61% over control), alongside a failure impact resistance of 1200.9 J (59 blows, a 78.8% increase). The static modulus ofelasticity reached 30.9 × 10³ N/mm², representing a 16.63% increase compared to the control mix. In aggressive chemicalenvironments, the optimum hybrid concrete exhibited superior resistance, restricting compressive strength loss to 15.64% in HCland 9.25% in MgSO₄, compared to 21.22% and 11.24% for conventional concrete. Overall, combining 10% Quartz Powder with1.0% Polypropylene Fiber optimizes structural performance while reducing OPC consumption by 34 kg/m³, offering a sustainable,high-performance concrete solution.Keywords: Cement Concrete, Quartz Powder, Polypropylene Fiber, Fiber-Reinforced Concrete, Compressive Strength,Impact Resistance, Modulus of Elasticity, Durability.
Authors
- Banavath Balaji Naik¹, D. V. Prasada Rao²
Publication Details
- Journal
- Zenodo (CERN European Organization for Nuclear Research)
- Published
- 2026-11-26
- DOI
- https://doi.org/10.5281/zenodo.24549779
- Primary Topic
- Innovative concrete reinforcement materials
- Type
- article
- Field-Weighted Citation Impact
- 0.00