Corrosion performance of structural steels and coated alloys under accelerated salt exposure

Corrosion significantly affects the durability and maintenance costs of metallic structures in saline environments. This study compared the corrosion behavior of ASTM A36 carbon steel, galvanized steel, aluminized steel, and 430F and 304L stainless steels under a six-week modified salt-spray exposure protocol incorporating daily heating (35 ± $$2^\circ $$ C, 5% NaCl saline solution) and cooling cycles. Specimens were positioned at $$30^\circ $$ and $$45^\circ $$, and corrosion was assessed through visual inspection and gravimetric measurements. Among the specimens tested, A36 exhibited the highest mass loss, whereas the coated steels showed intermediate values and the stainless steels the lowest. Differences between inclination angles were also observed, although the absence of independent replicates limits general conclusions. Expressing mass loss as a percentage of initial mass and per unit nominal surface area provided complementary measures of material degradation. The extended exposure period revealed changes in mass-loss trends after four weeks for the coated steels, highlighting the importance of monitoring corrosion over time.

Authors

Institutions

Publication Details

Journal
Journal of Materials Science Metallurgy
Published
2026-11-25
DOI
https://doi.org/10.1007/s44492-026-00029-7
Primary Topic
Corrosion Behavior and Inhibition
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Corrosion performance of structural steels and coated alloys under accelerated salt exposure

Leonardo Souza de Carvalho, Eduardo Marques Vieira, Rafael Pimentel Pigatti, Viviane Azambuja Favre Nicolin
3 links
Journal of Materials Science Metallurgy
Corrosion Behavior and Inhibition
article

Corrosion performance of structural steels and coated alloys under accelerated salt exposure

Leonardo Souza de Carvalho, Eduardo Marques Vieira, Rafael Pimentel Pigatti, Viviane Azambuja Favre Nicolin
article en

Abstract

Corrosion significantly affects the durability and maintenance costs of metallic structures in saline environments. This study compared the corrosion behavior of ASTM A36 carbon steel, galvanized steel, aluminized steel, and 430F and 304L stainless steels under a six-week modified salt-spray exposure protocol incorporating daily heating (35 ± $$2^\circ $$ C, 5% NaCl saline solution) and cooling cycles. Specimens were positioned at $$30^\circ $$ and $$45^\circ $$, and corrosion was assessed through visual inspection and gravimetric measurements. Among the specimens tested, A36 exhibited the highest mass loss, whereas the coated steels showed intermediate values and the stainless steels the lowest. Differences between inclination angles were also observed, although the absence of independent replicates limits general conclusions. Expressing mass loss as a percentage of initial mass and per unit nominal surface area provided complementary measures of material degradation. The extended exposure period revealed changes in mass-loss trends after four weeks for the coated steels, highlighting the importance of monitoring corrosion over time.

Journal of Materials Science MetallurgyVol. 1(1)
Instituto Federal do Espírito Santo (BR), Universidade Federal do Espírito Santo (BR)
Corrosion Behavior and Inhibition
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon