Mechanistic Aspects of Transitional Oxidic Middle‐Term Corrosion of Graphite Cast Iron in Wyoming Bentonite Slurry at 50°C: Electrochemical and Surface Chemistry Studies
The corrosion of spheroidal graphite cast iron GGG40 in a naturally aerated, saline Wyoming‐bentonite slurry at 50°C was monitored over the first 100 days using polarisation curves and impedance spectroscopy. Surface chemistry and morphological changes were investigated via SEM‐EDS and local XPS. The slurry substantially blocks the diffusion of dissolved oxygen to the cast iron surface. The reduction of minor amounts of oxygen that do reach the surface causes current fluctuations; these are superimposed on the base polarisation curves, which are dominated by water reduction. These fluctuations are interpreted as alternating cathodic and anodic events involving alkaline iron dissolution and the formation of passivating ferric hydroxide. Water reduction regulates the active dissolution of iron with a predominance of adsorbed H ads at the corrosion potential. Non‐passivating Fe(II, III) silicates and oxides grow at the interface during iron dissolution. Based on the chemical and morphological studies, it is highly probable that the former develops from ferrous hydroxide—acting as the primary corrosion product—alongside products of the alkaline dissolution of smectite.
Authors
- Dieter Schild (ORCID: https://orcid.org/0000-0001-6034-8146)
- Andrés Gabriel Muñoz (ORCID: https://orcid.org/0000-0002-5394-3390)
Institutions
- Karlsruhe Institute of Technology (DE)
- Kerntechnische Entsorgung Karlsruhe (Germany) (DE)
- Gesellschaft für Anlagen und Reaktorsicherheit (DE)
Publication Details
- Journal
- Materials and Corrosion
- Published
- 2026-11-25
- DOI
- https://doi.org/10.1002/maco.70321
- Primary Topic
- Corrosion Behavior and Inhibition
- Type
- article
- Field-Weighted Citation Impact
- 0.00
Funders
- European Commission
- Bundesministerium für Umwelt, Naturschutz, nukleare Sicherheit und Verbraucherschutz