Novel graphene oxide–silane nanocoatings on sound enamel: in vitro characterization and proof-of-principle assessment evaluation against erosive tooth wear

Objective This proof‑of‑principle study evaluated whether a novel graphene oxide (GO)–silane nanocoating applied to sound enamel can provide acid resistance under a standardized citric‑acid erosion model. Materials and Methods Ninety bovine enamel specimens were assigned into six groups: negative control, stannous-containing positive control, and four experimental coatings combining 3-methacryloxypropyltrimethoxysilane (MPS) with GO, with or without phosphoric acid pretreatment or stannous rinse. Surface characterization was performed by scanning electron microscopy (SEM). Following a 10-day erosive cycling protocol (six daily immersions in 1% citric acid, pH 2.3, surface loss was quantified on days 0, 4, 7, and 10 using optical profilometry (FRT). Data was analyzed using repeated-measures ANOVA. Results The GO-based coatings did not prevent enamel erosion. The positive control group consistently showed superior protective performance (surface loss: − 19.2 ± 3.6 µm; p < 0.05) over the negative control group (–29.3 ± 6.8 µm). GO-coated samples showed no protective effect, with mean enamel losses of − 32.9 ± 6.2 µm (only MPS), − 33.2 ± 3.7 µm (MPS + GO), and − 28.6 ± 6.7 µm (MPS + GO + stannous), showing no significant difference from the negative control (p > 0.05). Phosphoric acid pretreatment (phosphoric acid + MPS + GO) caused the highest substance loss (–39.7 ± 3.8 µm; p > 0.05). Conclusions GO–silane nanocoatings can be formed on enamel but do not confer resistance to citric-acid erosion. Phosphoric acid pretreatment compromises enamel integrity and should be avoided. Clinical Relevance: Current GO formulation and bonding approach do not provide erosion protection. Future development must optimize coupling agents and functionalized GO systems to achieve clinically meaningful acid resistance.

Authors

Institutions

Publication Details

Journal
Research Square
Published
2026-11-25
DOI
https://doi.org/10.21203/rs.3.rs-11701201/v1
Primary Topic
Dental Erosion and Treatment
Type
preprint
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
preprint

Novel graphene oxide–silane nanocoatings on sound enamel: in vitro characterization and proof-of-principle assessment evaluation against erosive tooth wear

Kamil Drożdż, Karolina Schickle, Esteves-Oliveira Marcella, Dina Abo-El-Lil
1 links
Research Square
Dental Erosion and Treatment
preprint

Novel graphene oxide–silane nanocoatings on sound enamel: in vitro characterization and proof-of-principle assessment evaluation against erosive tooth wear

Kamil Drożdż, Karolina Schickle, Esteves-Oliveira Marcella, Dina Abo-El-Lil
preprint en

Abstract

Objective This proof‑of‑principle study evaluated whether a novel graphene oxide (GO)–silane nanocoating applied to sound enamel can provide acid resistance under a standardized citric‑acid erosion model. Materials and Methods Ninety bovine enamel specimens were assigned into six groups: negative control, stannous-containing positive control, and four experimental coatings combining 3-methacryloxypropyltrimethoxysilane (MPS) with GO, with or without phosphoric acid pretreatment or stannous rinse. Surface characterization was performed by scanning electron microscopy (SEM). Following a 10-day erosive cycling protocol (six daily immersions in 1% citric acid, pH 2.3, surface loss was quantified on days 0, 4, 7, and 10 using optical profilometry (FRT). Data was analyzed using repeated-measures ANOVA. Results The GO-based coatings did not prevent enamel erosion. The positive control group consistently showed superior protective performance (surface loss: − 19.2 ± 3.6 µm; p < 0.05) over the negative control group (–29.3 ± 6.8 µm). GO-coated samples showed no protective effect, with mean enamel losses of − 32.9 ± 6.2 µm (only MPS), − 33.2 ± 3.7 µm (MPS + GO), and − 28.6 ± 6.7 µm (MPS + GO + stannous), showing no significant difference from the negative control (p > 0.05). Phosphoric acid pretreatment (phosphoric acid + MPS + GO) caused the highest substance loss (–39.7 ± 3.8 µm; p > 0.05). Conclusions GO–silane nanocoatings can be formed on enamel but do not confer resistance to citric-acid erosion. Phosphoric acid pretreatment compromises enamel integrity and should be avoided. Clinical Relevance: Current GO formulation and bonding approach do not provide erosion protection. Future development must optimize coupling agents and functionalized GO systems to achieve clinically meaningful acid resistance.

Research Square
Jagiellonian University (PL), Justus-Liebig-Universität Gießen (DE), Universitätsklinikum Tübingen (DE)
Good health and well-being
Dental Erosion and Treatment
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.