ДОСЛІДЖЕННЯ РУЙНУВАННЯ СТЕБЕЛ ЛЬОНУ ОЛІЙНОГО ДЛЯ ОБҐРУНТУВАННЯ РОБОЧИХ ПОВЕРХОНЬ ДЕКОРТИКАЦІЙНОГО ВУЗЛА
The deformation and fracture behaviour of groups of oilseed flax stems under quasi-static loading between profiled working surfaces was investigated. Laboratory tests were conducted using an extensometer fitted with an additional attachment equipped with interchangeable surfaces of triangular, circular and trapezoidal profiles. Each test series used a group of 20 stems, whose diameters were measured in the lower, middle and upper sections. Loading was applied sequentially at the corresponding sections of the same group. Displacement mechanism readings, indicator readings and instances of audible cracking accompanied by drops in the readings were recorded. Yellow stems and grey stems (retted straw) were tested separately using the circular profile. In all groups, the mean diameter decreased from the lower to the upper section. The loading records included intervals of increasing indicator readings, local drops followed by renewed increases, and intervals with little change in the readings. The results are presented in the original units of the readout devices, without conversion to force or actual displacement of the working surfaces. Comparisons between test series are descriptive and account for differences in geometric characteristics and material condition. The recorded relationships characterise the behaviour of the tested groups and provide a basis for refining the programme of further research into the working surfaces of a decortication unit.
Authors
- Р.А. Хлопецький
- В.Ф. Дідух
Institutions
- Lutsk National Technical University (UA)
Publication Details
- Journal
- СІЛЬСЬКОГОСПОДАРСЬКІ МАШИНИ
- Published
- 2026-11-26
- DOI
- https://doi.org/10.36910/acm.vi52.2340
- Primary Topic
- Agricultural Engineering and Mechanization
- Type
- article
- Field-Weighted Citation Impact
- 0.00