Evolution of Sidewall Penetration and Weld-Pool Dynamics in Narrow-Gap Gas Tungsten Arc Welding of Thick TC4 Titanium Alloy Plate
In welding of thick titanium alloy plates, welding parameters exert a significant influence on the dynamic behavior of the weld pool. In thick-plate welding, lack of sidewall fusion is a predominant welding defect. In this study, experiments were conducted under varying welding parameters for TIG (Tungsten Inert Gas Welding) wire-filling welding of thick titanium alloy plates. A multi-physics weld pool model was established to investigate the influence of welding parameters on the dynamic behavior characteristics of the weld pool, as well as the mechanisms through which welding parameters contribute to lack of sidewall fusion. The numerical results show that, during the welding process, the dynamic behavior characteristics of the weld pool do not vary significantly between different weld passes. When the welding current is excessively high, or the welding speed is excessively fast, the defect of lack of sidewall fusion becomes pronounced. The numerical predictions are qualitatively consistent with the experimentally observed trends in sidewall penetration.
Authors
- Qianli Liu
- Haibin Liu
- Wenyong Zhao
- Enyang Fan (ORCID: https://orcid.org/0009-0002-9042-5362)
- Jingyu Liu
- Guoxiang Xu
Institutions
- Jiangsu University of Science and Technology (CN)
- Luoyang Ship Material Research Institute (CN)
Publication Details
- Journal
- Metals
- Published
- 2026-11-25
- DOI
- https://doi.org/10.3390/met16121300
- Primary Topic
- Welding Techniques and Residual Stresses
- Type
- article
- Field-Weighted Citation Impact
- 0.00