Membrane, Air, and Water Curing of GGBS and Microsilica Concrete: Age-Dependent Strength Penalty and Carbon Cost
In water-scarce regions, curing water is often desalinated, yet curing of blended concrete is judged on 28-day strength. We tested whether this holds for ordinary Portland cement (OPC), 50% ground granulated blast furnace slag (GGBS), and 7% microsilica (MS) concretes cured in water or exposed outdoors for 20 days, bare or under a membrane-forming curing compound, and whether water curing repays its carbon cost. Strength was measured at 7, 28 and 90 days, alongside absorption, sorptivity, microstructure, and a life-cycle assessment including curing. The curing penalty reversed with age: GGBS concrete was most affected at 7 days (retention 0.63–0.64) but recovered to 0.89–0.96, whereas MS concrete retained 0.94–0.95 at 28 days and fell to 0.83–0.85 at 90 days. A Eurocode 2-type function fitted at 7 and 28 days predicted 90-day water-cured strength within 7% but erred by up to 18% for non-water-cured blended concrete. Desalinated curing water added at most 2.4% to global warming potential per cubic meter, whereas non-water curing raised it per MPa by up to 28%; except for OPC at 7 days, water curing stayed lower-carbon unless its burden was 1.9–24 times higher. Blended-concrete curing should be specified per binder and verified beyond 28 days.
Authors
- Jacqueline Saliba (ORCID: https://orcid.org/0000-0001-6648-5520)
- Christelle Tohme (ORCID: https://orcid.org/0009-0005-3112-2961)
- Yasmeen Alrasheedi
- Rayan Aljabaah
- Farah Alazmi
- Wadhha Alotaibi
- Shahad Alghanim
Institutions
- American University of the Middle East (KW)
Publication Details
- Journal
- Coatings
- Published
- 2026-11-25
- DOI
- https://doi.org/10.3390/coatings16121400
- Primary Topic
- Concrete and Cement Materials Research
- Type
- article
- Field-Weighted Citation Impact
- 0.00