Engineering Si─O─C Active Units by Bisphenol A Toward High‐Capacity SiOC Anodes for Lithium‐Ion Batteries
Silicon oxycarbide ceramics hold great promise as lithium‐ion battery anodes by virtue of their elevated theoretical capacity and robust structural stability. Crucially, the electrochemical behavior of SiOC is governed by the content of SiO 3 C and SiO 2 C 2 units within its amorphous Si─O─C network. In this work, bisphenol A was employed to modulate the condensation process between phenolic hydroxyl groups and silanols. This strategy successfully accelerates the generation of Si─O─Si and Si─O─C networks, thereby enabling precise control over both the composition and microstructural architecture of the resulting SiOC ceramics. Characterization insights reveal that incorporating an optimal dosage of bisphenol A effectively reinforces the Si─O─C framework, elevating the collective fraction of SiO 3 C and SiO 2 C 2 units from 73.01% to 78.14%. Owing to the optimized structural composition, the fabricated SiOC‐2% anode delivers a reversible capacity reaching 1243.41 mAh g −1 at 0.1 A g −1. Additionally, a high capacity of approximately 974.9 mAh g −1 is sustained after 300 cycles at 0.5 A g −1. Remarkably, even at an aggressive rate of 4.0 A g −1, the anode still delivers 343.0 mAh g −1 after 1000 cycles, demonstrating an outstanding capacity retention of 86.4%.
Authors
- W. J. Liu (ORCID: https://orcid.org/0009-0006-3959-9091)
- Zhengwei Xie (ORCID: https://orcid.org/0000-0002-0542-0317)
- Shaoxiang Su
- Jingjing Gao
- Jiajia Weng
- Kun Chen
Institutions
- Chinese Academy of Sciences (CN)
- Chengdu Organic Chemicals (China) (CN)
- University of Chinese Academy of Sciences (CN)
Publication Details
- Journal
- ChemistrySelect
- Published
- 2026-11-25
- DOI
- https://doi.org/10.1002/slct.75243
- Primary Topic
- Lithium- and Sodium-Ion Battery Electrodes
- Type
- article
- Field-Weighted Citation Impact
- 0.00