Experimental investigation and 3D microstructural characterization of alkali-activated slag–trass blends supported by DFT calculations

The high-volume use of natural pozzolans could reduce the dependence of alkali-activated binders on geographically constrained blast-furnace slag (BFS) supplies, but their limited ambient-temperature reactivity often restricts mechanical performance. This study evaluates highly reactive artificial slag (AS), relative to conventional BFS, for improving the activation kinetics and strength development of mortars containing high-volume trass, a natural volcanic pozzolan. At an AS-to-untreated-trass ratio of 30:70 by volume and a Na 2 Oeq dosage of 5 wt% relative to the total dry mass of slag and trass, the Na 2 SiO 3 -activated mortar reached a 1-d compressive strength of 38 MPa, approximately ten times that of its BFS-based counterpart. At 90 d, the AS- and BFS-based mortars with 70 vol% of trass reached 77 and 65 MPa, respectively. The superior early performance of AS was associated with its higher Ca/Si and Al/Si ratios, which promoted rapid activation and formation of a mechanically effective binding matrix. Incorporating trass thermally treated at 500 °C increased the 90-d strength in the AS- and BFS-based mortars by ∼13% and ∼32%, respectively. Conversely, treating trass at 1000 °C substantially increased crystallinity, reduced reaction-product formation and workability as well as decreased compressive strength. Supporting density functional theory (DFT) calculations indicated a stronger affinity of the simplified alkaline solution for sanidine and analcime than for orthoclase and muscovite. These results provided a qualitative molecular-scale interpretation of the relative interfacial affinity of the selected crystalline minerals but did not quantify dissolution, reaction extent, or strength development. Overall, highly reactive AS compensated for the slow ambient-temperature activation of high-volume trass, while the experimental results demonstrated the combined influence of slag reactivity, trass mineralogy, and three-dimensional microstructural organization.

Authors

Institutions

Publication Details

Journal
Cement and Concrete Composites
Published
2026-11-25
DOI
https://doi.org/10.1016/j.cemconcomp.2026.106906
Primary Topic
Concrete and Cement Materials Research
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Experimental investigation and 3D microstructural characterization of alkali-activated slag–trass blends supported by DFT calculations

Yanliang Ji, Hamdy A. Abdel‐Gawwad, Dietmar A. Stephan, Hussein Al-kroom et al.
Cement and Concrete Composites
Concrete and Cement Materials Research
article

Experimental investigation and 3D microstructural characterization of alkali-activated slag–trass blends supported by DFT calculations

Yanliang Ji, Hamdy A. Abdel‐Gawwad, Dietmar A. Stephan, Hussein Al-kroom, Mohamed Abd Elrahman, Se-Yun Kim, C.W. Lehmann
article en

Abstract

The high-volume use of natural pozzolans could reduce the dependence of alkali-activated binders on geographically constrained blast-furnace slag (BFS) supplies, but their limited ambient-temperature reactivity often restricts mechanical performance. This study evaluates highly reactive artificial slag (AS), relative to conventional BFS, for improving the activation kinetics and strength development of mortars containing high-volume trass, a natural volcanic pozzolan. At an AS-to-untreated-trass ratio of 30:70 by volume and a Na 2 Oeq dosage of 5 wt% relative to the total dry mass of slag and trass, the Na 2 SiO 3 -activated mortar reached a 1-d compressive strength of 38 MPa, approximately ten times that of its BFS-based counterpart. At 90 d, the AS- and BFS-based mortars with 70 vol% of trass reached 77 and 65 MPa, respectively. The superior early performance of AS was associated with its higher Ca/Si and Al/Si ratios, which promoted rapid activation and formation of a mechanically effective binding matrix. Incorporating trass thermally treated at 500 °C increased the 90-d strength in the AS- and BFS-based mortars by ∼13% and ∼32%, respectively. Conversely, treating trass at 1000 °C substantially increased crystallinity, reduced reaction-product formation and workability as well as decreased compressive strength. Supporting density functional theory (DFT) calculations indicated a stronger affinity of the simplified alkaline solution for sanidine and analcime than for orthoclase and muscovite. These results provided a qualitative molecular-scale interpretation of the relative interfacial affinity of the selected crystalline minerals but did not quantify dissolution, reaction extent, or strength development. Overall, highly reactive AS compensated for the slow ambient-temperature activation of high-volume trass, while the experimental results demonstrated the combined influence of slag reactivity, trass mineralogy, and three-dimensional microstructural organization.

Cement and Concrete CompositesVol. 176
University of Jordan (JO), Mansoura University (EG), Housing and Building National Research Center (EG), Technische Universität Berlin (DE)
Concrete and Cement Materials Research
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon