Cathode-Generated Hydrogen Peroxide Contributes to Degradation of the Membrane Across Its Full Thickness in PEM Water Electrolyzers

Proton-exchange membrane (PEM) water electrolyzers must operate for 80,000 h, and membrane degradation limits this lifetime. Because electroosmotic drag carries degradation products toward the cathode, the fluoride emission rate, the standard diagnostic, underrepresents anode-side and bulk degradation. It also misses larger fluorocarbon fragments (LC-MS); after correction for compression, about 80% of the excess measured thinning (SEM) over fluoride-derived thinning at 1 A cm−2 is chemical loss. Depth profiles at both membrane faces in time-of-flight secondary ion mass spectrometry, with transport analysis, indicate anisotropic degradation across the full PEM thickness, consistent with cathode-generated hydrogen peroxide diffusing toward the anode, most strongly at 0.5–1.0 A cm−2. The estimated peroxide production rate is six times the molar rate of membrane loss. To reach 80,000 h, our results point to two design targets: oxygen crossover an order of magnitude below today's 1% benchmark, and peroxide-decomposition catalysts distributed throughout the membrane bulk.

Authors

Institutions

Publication Details

Journal
ACS Energy Letters
Published
2026-11-25
DOI
https://doi.org/10.1021/acsenergylett.6c02741
Primary Topic
Fuel Cells and Related Materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Cathode-Generated Hydrogen Peroxide Contributes to Degradation of the Membrane Across Its Full Thickness in PEM Water Electrolyzers

Zeyan Liu, Kuldeep Mamtani, Ke Xie, Edward Hartley Sargent et al.
ACS Energy Letters
Fuel Cells and Related Materials
article

Cathode-Generated Hydrogen Peroxide Contributes to Degradation of the Membrane Across Its Full Thickness in PEM Water Electrolyzers

Zeyan Liu, Kuldeep Mamtani, Ke Xie, Edward Hartley Sargent, Habin Park, Yoon Jun Son, W.T. Liu, Mengjie Liu, Zhaoping Shi
article en

Abstract

Proton-exchange membrane (PEM) water electrolyzers must operate for 80,000 h, and membrane degradation limits this lifetime. Because electroosmotic drag carries degradation products toward the cathode, the fluoride emission rate, the standard diagnostic, underrepresents anode-side and bulk degradation. It also misses larger fluorocarbon fragments (LC-MS); after correction for compression, about 80% of the excess measured thinning (SEM) over fluoride-derived thinning at 1 A cm−2 is chemical loss. Depth profiles at both membrane faces in time-of-flight secondary ion mass spectrometry, with transport analysis, indicate anisotropic degradation across the full PEM thickness, consistent with cathode-generated hydrogen peroxide diffusing toward the anode, most strongly at 0.5–1.0 A cm−2. The estimated peroxide production rate is six times the molar rate of membrane loss. To reach 80,000 h, our results point to two design targets: oxygen crossover an order of magnitude below today's 1% benchmark, and peroxide-decomposition catalysts distributed throughout the membrane bulk.

ACS Energy Letters
Northwestern University (US), Shell (United States) (US)
Fuel Cells and Related Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon