铝箔集流体的 Al/C 共溅射改性
Aluminum foil is the standard current collector for LiFePO₄ (LFP) cathodes, yet its interfacial failure has long been treated as a processing issue rather than a scientific one. This review surveys the 2015–2025 literature along three lines: low-potential lithiation of Al and the instability associated with the AlLi phase transformation; the role of carbon coatings in regulating interfacial charge transport; and the oxidation of sputtered Al during electrode drying. Three points are made. First, over-discharging an LFP cell to 2.0 V does not by itself trigger AlLi formation—cell reversal and local potential overshoot are the dominant causes, and the boundary between them can be delimited by a potential threshold combined with a characteristic lithiation time. Second, the irreversibility widely reported for Al–Li alloying is a mechanical consequence of transformation strain coupled with interfacial delamination, not a thermodynamic one. Third, because carbon-coating studies rely almost universally on binary coated/uncoated comparisons, they cannot separate electronic bridging from field uniformization. On this basis, we argue that the value of Al/C co-sputtering lies in its orthogonal tunability, and propose an "oxidation window" hypothesis: a dispersed 1–2 nm AlOₓ shell may deliver low contact resistance and high corrosion resistance simultaneously.
Authors
- 国平 刘
- 志佳 张
- 耀威 王
- 宇璇 孟
Institutions
- Tiangong University (CN)
- State Key Laboratory of Separation Membranes and Membrane Processes (CN)
Publication Details
- Journal
- 应用科技研究
- Published
- 2026-11-24
- DOI
- https://doi.org/10.68070/tvw1mz75
- Primary Topic
- Lithium- and Sodium-Ion Battery Electrodes
- Type
- article
- Field-Weighted Citation Impact
- 0.00