Effect of cyclic annealing and thermal oxidation on the oxidation kinetics, mechanical and microstructural properties of titanium--nickel (TiNi) alloys
This study evaluates the impact of cyclic annealing and thermal oxidation (650°C for 112 hours) on six powder metallurgy TiNi alloys containing 5–30 % by mass Ni. Oxidation kinetics strictly followed the parabolic rate law (R = 0.862 to 0.972). Parabolic rate constants (kp) decreased from 0.0012 mg²/mm⁴·s for Ti-5% by mass Ni to 4 × 10−6 mg²/(mm⁴·s) for Ti-25% by mass Ni, confirming exceptional high-temperature oxidation resistance. Structural analyses using XRD and FESEM-EDS confirmed the growth of a dense, protective surface oxide scale composed primarily of stable rutile TiO₂. This ceramic layer acts as a robust diffusion barrier, preventing outward nickel ion migration and significantly improving alloy biocompatibility. Mechanically, the thermal treatment enhanced surface microhardness, increasing Vickers hardness by 28.3% (915 HV) in Ti-5% by mass Ni and 31.9% (804.6 HV) in Ti-30% by mass Ni, while Ti-15% by mass Ni maintained a stress-relieved 741.6 HV. Overall, precise thermal processing and compositional control optimize TiNi alloys for advanced biomedical and engineering applications.
Authors
- Sheamaa Al-Dbag
Publication Details
- Journal
- OCHRONA PRZED KOROZJĄ
- Published
- 2026-11-24
- DOI
- https://doi.org/10.15199/40.2026.11.2
- Primary Topic
- Titanium Alloys Microstructure and Properties
- Type
- article
- Field-Weighted Citation Impact
- 0.00