Effect of Mn-Doping on Sodium Niobate Bismuth Ferrite Ceramics and PLD Thin Films for Energy Storage Applications
Sodium niobate (NaNbO3) is a well-researched perovskite. In 2021 Jiang and colleagues demonstrated how the introduction of bismuth ferrite (BiFeO3) stabilized the sodium niobate AFE phase and induced relaxor-like behavior. The relaxor-like behavior results from the Bi3+ and Fe3+ disrupting the long-range antiferroelectric orders in the sodium niobate matrix, which decreases the domain size and enhances the relaxor-like behavior. It was found that the 0.9(NaNbO3) – 0.1(BiFeO3) had the optimal energy storage properties (Wrec=18.5 J/cm3, η=78.7%, Eb=995 kV/cm). Additionally, the efficiency of this composition is somewhat low. The energy loss (Wloss) stems from the area inside of the hysteresis curve, which originates from leakage current within the material. Doping with manganese oxide (MnO2) has been shown to reduce high-field leakage current in other perovskite oxides like BNT-BKT as well KNN, which is very similar to this NN based system. Therefore, the effects of Mn-doping should be explored to understand its effects on the leakage current of the 0.9NN-0.1BF composition. Ceramics with x% Mn4+ of the (Na0.9Bi0.1)(Nb0.9Fe0.1-(4/3)xMnx)O3 (x = 0, 1.25, 1.50, 1.75) (abbreviated at NN-BF, 1.25Mn:NN-BF, 1.5Mn:NN-BF, 1.75Mn:NN-BF) composition were synthesized using the conventional oxide route. High-energy planetary milling was performed after calcination to reduce the calcined powder particle size and improve ceramic density and decrease grain size. All compositions were calcined at 900 °C for 3 hours and sintered at 1150 °C in a box furnace. The Mn-doped ceramics had a smaller average grain size and slimmer grain size distribution compared to the pure ceramics, perhaps due to increased lattice diffusion with the introduction of Mn. The εr and tan δ of all ceramic compositions were comparable to each other and consistent with the literature. At high fields, Mn-doped ceramics exhibited higher leakage current compared to pure NN-BF ceramics. The 1.5Mn:NN-BF composition had the best energy storage properties, with Emax= 280 kV/cm, Wrec = 3.043 J/cm3, and η=94.9%. The breakdown of all compositions is significantly lower than previously reported values. The lower breakdown strength compared to the literature is attributed to a second phase shown in optical micrographs of the ceramics. The lower breakdown of Mn-doped ceramics is most likely due to the introduction of oxygen vacancies in the ceramics, which act as a pathway for conduction. At this time, there are no studies that have investigated the energy storage properties of NN-BF films, prepared by any technique. PLD is a promising starting point to explore the synthesis of NN-BF films due to the high tunability of the processing technique. Due to volatility of both Na3+ and Bi3+, the phase structure and elemental composition of the films are to be examined as a function of film processing parameters. Finally, the effect of Mn-doping on the films is compared to the electrical properties of the bulk ceramics to further understand how these materials are to be improved. ~100 nm NN-BF thin films were grown on single crystal SrTiO3 (001) substrates by Pulsed Laser Deposition (PLD). Film growth was optimized based on morphology, phase, and chemistry by tuning the laser fluence, deposition temperature, and oxygen partial pressure. A change in the laser fluence had a large effect on the ablated target microstructure but did not significantly change the deposited films. Deposition temperature affected film morphology, with higher temperatures showing smoother microstructures. Oxygen partial pressure had a significant effect on plume geometry and the resulting film stoichiometry. Most notably, Na-content decreased with increasing oxygen partial pressure. Based on the investigation of processing parameters, optimized values for laser fluence, deposition temperature, and oxygen partial pressure were 2.0 J/cm2, 600 °C, and 300 mTorr O2, respectively. The optimized films had correct phase and were highly oriented and a smooth surface morphology. Additionally, the films were roughly stoichiometric, however RBS and XPS measurements both showed that the films were slightly bismuth-deficient due to slow transport kinetics. Optimized thin films of NN-BF, 1.25Mn:NN-BF, 1.5Mn:NN-BF, and 1.75Mn:NN-BF composition with thickness ~100 nm were grown on Nb:STO (100) for electrical evaluation. A post deposition annealing at 400 °C for 1 h in 1 atm O2 significantly reduced the leakage current of all films. At RT, the NN-BF, 1.25Mn:NN-BF, and 1,5Mn:NN-BF compositions all showed an εr and tan δ around 450 and 3.5% while the εr and tan δ of the 1,75Mn:NN-BF composition was about 400 and 2% from 1 kHz to 1 MHz. All compositions exhibited a slight decrease in εr and tan δ with increasing frequency. At high-fields, the Mn-doped films demonstrated lower Pr than pure NN-BF films. Energy storage properties were maximized for the 1.5Mn:NN-BF composition with a Wrec of 2.22 J/cm3. Mn-doping significantly reduced the leakage current of the films. The leakage current greater than 1 order of magnitude for all Mn-doped compositions. The similar leakage current suggests that a saturation point is reached to optimize the reduced leakage current effect of the manganese.
Authors
- Adam Steven Wynne
Publication Details
- Journal
- Rutgers University Community Repository (Rutgers University)
- Published
- 2026-11-24
- DOI
- https://doi.org/10.7282/t3-1abg-ce30
- Primary Topic
- Ferroelectric and Piezoelectric Materials
- Type
- article
- Field-Weighted Citation Impact
- 0.00