A multiscale assessment of DEF development and damage in concrete: Effects of initial curing temperature and SCMs

Delayed ettringite formation (DEF) remains a relevant durability concern in concrete exposed to elevated temperatures at early ages, particularly when supplementary cementitious materials (SCMs) are used and may modify the kinetics and expression of deterioration. This study investigates the influence of initial curing temperature and binder composition on the long-term development of DEF in concretes produced with high-early-strength Portland cement, 35% fly ash, and 50% ground granulated blast-furnace slag. Specimens were thermally cured at 60, 70, or 85°C and subsequently stored in water at 38°C for up to 545 days. DEF progression was evaluated through expansion monitoring, conventional mechanical properties, direct shear strength, Damage Rating Index (DRI), X-ray computed tomography, and SEM/EDS observations. The reference concrete cured at 85°C exhibited the most severe response, reaching 0.21% expansion at 545 days, together with reductions of approximately 36% in compressive strength, 29% in splitting tensile strength, 25% in modulus of elasticity, and 17% in direct shear strength between 180 and 545 days. Fly ash substantially reduced expansion and delayed mechanical deterioration, although late-age losses were still observed under the most severe curing condition. GGBFS limited expansion to approximately 0.03% and preserved conventional mechanical properties, while DRI indicated only limited internal distress. The comparison among binder systems showed that similar expansion levels did not necessarily correspond to equivalent damage states. These findings highlight that DEF deterioration cannot be reliably interpreted from expansion alone, particularly in SCM concretes, and reinforce the need for an integrated multiscale assessment combining macroscopic, mechanical, and microstructural indicators.

Authors

Institutions

Publication Details

Journal
Construction and Building Materials
Published
2026-11-24
DOI
https://doi.org/10.1016/j.conbuildmat.2026.148962
Primary Topic
Concrete Properties and Behavior
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

A multiscale assessment of DEF development and damage in concrete: Effects of initial curing temperature and SCMs

R. H. R. Q. Melo, Nicole Pagan Hasparyk, Denise Carpena Coitinho Dal Molin, Juliane Rodrigues Falcão
1 links
Construction and Building Materials
Concrete Properties and Behavior
article

A multiscale assessment of DEF development and damage in concrete: Effects of initial curing temperature and SCMs

R. H. R. Q. Melo, Nicole Pagan Hasparyk, Denise Carpena Coitinho Dal Molin, Juliane Rodrigues Falcão
article en

Abstract

Delayed ettringite formation (DEF) remains a relevant durability concern in concrete exposed to elevated temperatures at early ages, particularly when supplementary cementitious materials (SCMs) are used and may modify the kinetics and expression of deterioration. This study investigates the influence of initial curing temperature and binder composition on the long-term development of DEF in concretes produced with high-early-strength Portland cement, 35% fly ash, and 50% ground granulated blast-furnace slag. Specimens were thermally cured at 60, 70, or 85°C and subsequently stored in water at 38°C for up to 545 days. DEF progression was evaluated through expansion monitoring, conventional mechanical properties, direct shear strength, Damage Rating Index (DRI), X-ray computed tomography, and SEM/EDS observations. The reference concrete cured at 85°C exhibited the most severe response, reaching 0.21% expansion at 545 days, together with reductions of approximately 36% in compressive strength, 29% in splitting tensile strength, 25% in modulus of elasticity, and 17% in direct shear strength between 180 and 545 days. Fly ash substantially reduced expansion and delayed mechanical deterioration, although late-age losses were still observed under the most severe curing condition. GGBFS limited expansion to approximately 0.03% and preserved conventional mechanical properties, while DRI indicated only limited internal distress. The comparison among binder systems showed that similar expansion levels did not necessarily correspond to equivalent damage states. These findings highlight that DEF deterioration cannot be reliably interpreted from expansion alone, particularly in SCM concretes, and reinforce the need for an integrated multiscale assessment combining macroscopic, mechanical, and microstructural indicators.

Construction and Building MaterialsVol. 552
Universidade Federal do Rio Grande do Sul (BR)
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior
Concrete Properties and Behavior
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon