Phosphogypsum valorization in clay-based flat ceramic membranes for tannery wastewater treatment
Tannery wastewater is characterized by high turbidity, intense coloration, elevated organic load, and the presence of colloidal and recalcitrant pollutants, making its treatment a persistent environmental challenge. Conventional treatment methods often fail to meet discharge limits due to the complex composition of tannery effluents, highlighting the need for robust and chemically stable filtration materials such as ceramic membranes. In this study, the chemical, thermal, structural, and morphological characteristics of phosphogypsum (PG) and clay were comprehensively analyzed using XRF, TGA, FTIR, XRD, SEM, and particle size analysis (PSA), providing essential insights into their composition and phase evolution for ceramic membrane fabrication. Ceramic membranes were prepared by incorporating different PG contents (3, 5, 7, and 9 wt%) into a clay matrix, followed by shaping with a hydraulic press and sintering at 1100 °C. The influence of PG, a pore-forming agent, on key membrane properties, including porosity, microstructure, and mechanical strength, was systematically investigated. The ceramic membrane incorporating 9 wt% PG was identified as the optimal composition, meeting the required specifications with an open porosity of 47.9% and an indirect tensile strength of 10.94 MPa. The optimized membrane exhibited a high-water permeability of about 1160 L·h⁻¹ ·m⁻²·bar⁻¹ and effectively clarified tannery beamhouse effluent, achieving a turbidity rejection of 99.05% and a color removal of about 69%. It also reduced the chemical oxygen demand (COD) by about 84%. Fouling analysis indicated that the flux decline was not governed by a single mechanism: intermediate pore blocking predominated during the initial stage of filtration, followed by an increasing contribution of cake layer formation as filtration proceeded. After a single alkaline cleaning cycle, the membrane recovered about 57% of its initial water permeability; it showed a low mass loss in alkaline medium (< 0.23% after 250 h in 1 M NaOH) but a higher mass loss in acidic medium (about 4.5% in 1 M HNO₃).
Authors
- Abdelmjid Bouazizi (ORCID: https://orcid.org/0000-0003-3588-1998)
- Mossaab Mouiya (ORCID: https://orcid.org/0000-0002-2470-6433)
- Y. Abouliatim (ORCID: https://orcid.org/0000-0003-3463-8427)
- Mhammed El Kouali (ORCID: https://orcid.org/0000-0002-7036-450X)
- Abdelkrim Abourriche (ORCID: https://orcid.org/0009-0003-6852-8311)
- Yassine Rakcho (ORCID: https://orcid.org/0000-0002-9264-158X)
- Laila Bennani
- Sara Bouk
- Ayoub Lahmidi
Institutions
- Cadi Ayyad University (MA)
- Centre National de la Recherche Scientifique (FR)
- Jadara University (JO)
- Institut de Recherche sur les Céramiques (FR)
- Université Moulay Ismail de Meknes (MA)
- Instituto Superior da Maia (PT)
- Université de Limoges (FR)
- University of Hassan II Casablanca (MA)
Publication Details
- Journal
- Next Materials
- Published
- 2026-11-25
- DOI
- https://doi.org/10.1016/j.nxmate.2026.104126
- Primary Topic
- Recycling and utilization of industrial and municipal waste in materials production