Post-fabrication dispersion trimming of thin-film lithium niobate waveguides with segmented Sb2S3 claddings
Group-velocity dispersion in thin-film lithium niobate is set by the film thickness to the nanometre: an 8 nm thickness error, within commercial wafer tolerances, shifts β2 at 1550 nm by about 28 ps²/km. Here, we show in simulations that a segmented, non-volatile Sb2S3 cladding can correct this error after fabrication. Four independently switched binary segments reach a two-dimensional region of the (β2,β3) plane. Because the segment states shift with the die error, the bit pattern is chosen from a per-die spectral surrogate constrained by exact identities of the lossless Maxwell problem, with the die error read from two test rings. Scored on full-wave solutions, this procedure trims 96.8% of the dies into ±25 ps²/km. This work offers a route to post-fabrication dispersion correction for dispersion-engineered nonlinear devices such as microcombs and parametric amplifiers.
Authors
- Shoumik Debnath (ORCID: https://orcid.org/0009-0001-9500-5319)
- Sudipta Saha (ORCID: https://orcid.org/0009-0003-9110-8059)
- Anup Modak
Publication Details
- Published
- 2026-11-24
- DOI
- https://doi.org/10.1364/opticaopen.35097967
- Primary Topic
- Photorefractive and Nonlinear Optics
- Type
- preprint