EFFECT OF PROCESSING PARAMETERS ON THE ENERGY STORAGE PROPERTIES OF SODIUM NIOBATE BISMUTH FERRITE CERAMICS

Relaxor antiferroelectric (AFE) Electroceramics are excellent candidates for energy storage applications due to their high efficiency and recoverable energy and low remnant polarization. NaNbO3 is a promising lead-free antiferroelectric due to its high band gap, breakdown field and polarizability. However, it faces issues due to the co-existence of ferroelectric phases at standard temperature, pressure and electric field conditions, reducing its energy storage properties. This issue can be mitigated by the addition of other perovskites, which can stabilize the AFE phase, induce relaxor behavior and improve energy storage properties. Among the NaNbO3-based solid solution, .9NaNbO3-.1BiFeO3 is an especially promising composition studied by Jiang et. al. who reported high recoverable energy storage of 18.5 J/cm3 and ultra-high breakdown field of 995 kV/cm in bulk ceramics. However, these results have not been reproducible and a previously unreported second phase has also been discovered in this composition that might be hindering its energy storage properties. It is hypothesized that the secondary phase is resulting from impurity phases formed during the synthesis of BiFeO3 from Bi2O3 and Fe2O3 via mixed oxide calcination. In this study, .9NaNbO3-.1BiFeO3 ceramic powder was synthesized using a Mixed Oxide calcination method to replicate the results of the original study. The same starting oxide compositions, binder, calcination and sintering conditions were used to duplicate the study as closely as possible. Additionally, further experiments were performed to optimize the energy storage properties of the material. Next, a Rapid Liquid Calcination (RLC) method was utilized to synthesize pure phase BiFeO3, as confirmed by XRD, SEM, EDS and optical microscopy analysis. Finally, the pure phase BiFeO3 and NaNbO3 were mixed together via the Perovskite method of calcination. It was found that using high energy ball milling for 12 hours at 350 RPM reduces the particle size of .9NaNbO3-.1BiFeO3 powder to an average of .770µm and produces highly dense sintered ceramics. It was also found that the addition of 0.7 wt% PVA binder and applying 10 MPA pressing pressure on the greenbodies produces the highest density samples and significantly reduces the risk of delamination or porosity. The use of ultra-high purity starting oxide powders actually decreased the energy storage properties of .9NaNbO3-.1BiFeO3, and conventionally pure starting oxides that typically contained ~.1% impurities gave significantly better results. Following these processing parameters, the Mixed Oxide method samples produced bulk ceramics that had a Wrec = 8.18 J/cm3, Eb = 570 kV/cm and η = 67.8%. Pure BiFeO3 was produced using an optimized rapid liquid calcination process where the powder was rapidly heated to 880C, heated for 30 min, then rapidly quenched to room temperature. In addition to using the RLC method, it was also necessary to add 2.5 wt% excess Bi2O3 to control Bi volatility as well as 1 wt% Nb2O5 and Na2CO3 powders to stabilize the pure BiFeO3 phase. This powder was used to produce .9NaNbO3-.1BiFeO3 using the Perovskite method. It was found that the secondary phase was still present in the Perovskite method ceramics, which had a Wrec = 2.82 J/cm3, Eb = 320 kV/cm and η = 75.9%.

Authors

Publication Details

Journal
Rutgers University Community Repository (Rutgers University)
Published
2026-11-24
DOI
https://doi.org/10.7282/t3-4npa-3188
Primary Topic
Ferroelectric and Piezoelectric Materials
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

EFFECT OF PROCESSING PARAMETERS ON THE ENERGY STORAGE PROPERTIES OF SODIUM NIOBATE BISMUTH FERRITE CERAMICS

Sreeakhil Pulipaka
4 links
Rutgers University Community Repository (Rutgers University)
Ferroelectric and Piezoelectric Materials
article

EFFECT OF PROCESSING PARAMETERS ON THE ENERGY STORAGE PROPERTIES OF SODIUM NIOBATE BISMUTH FERRITE CERAMICS

Sreeakhil Pulipaka
article en

Abstract

Relaxor antiferroelectric (AFE) Electroceramics are excellent candidates for energy storage applications due to their high efficiency and recoverable energy and low remnant polarization. NaNbO3 is a promising lead-free antiferroelectric due to its high band gap, breakdown field and polarizability. However, it faces issues due to the co-existence of ferroelectric phases at standard temperature, pressure and electric field conditions, reducing its energy storage properties. This issue can be mitigated by the addition of other perovskites, which can stabilize the AFE phase, induce relaxor behavior and improve energy storage properties. Among the NaNbO3-based solid solution, .9NaNbO3-.1BiFeO3 is an especially promising composition studied by Jiang et. al. who reported high recoverable energy storage of 18.5 J/cm3 and ultra-high breakdown field of 995 kV/cm in bulk ceramics. However, these results have not been reproducible and a previously unreported second phase has also been discovered in this composition that might be hindering its energy storage properties. It is hypothesized that the secondary phase is resulting from impurity phases formed during the synthesis of BiFeO3 from Bi2O3 and Fe2O3 via mixed oxide calcination. In this study, .9NaNbO3-.1BiFeO3 ceramic powder was synthesized using a Mixed Oxide calcination method to replicate the results of the original study. The same starting oxide compositions, binder, calcination and sintering conditions were used to duplicate the study as closely as possible. Additionally, further experiments were performed to optimize the energy storage properties of the material. Next, a Rapid Liquid Calcination (RLC) method was utilized to synthesize pure phase BiFeO3, as confirmed by XRD, SEM, EDS and optical microscopy analysis. Finally, the pure phase BiFeO3 and NaNbO3 were mixed together via the Perovskite method of calcination. It was found that using high energy ball milling for 12 hours at 350 RPM reduces the particle size of .9NaNbO3-.1BiFeO3 powder to an average of .770µm and produces highly dense sintered ceramics. It was also found that the addition of 0.7 wt% PVA binder and applying 10 MPA pressing pressure on the greenbodies produces the highest density samples and significantly reduces the risk of delamination or porosity. The use of ultra-high purity starting oxide powders actually decreased the energy storage properties of .9NaNbO3-.1BiFeO3, and conventionally pure starting oxides that typically contained ~.1% impurities gave significantly better results. Following these processing parameters, the Mixed Oxide method samples produced bulk ceramics that had a Wrec = 8.18 J/cm3, Eb = 570 kV/cm and η = 67.8%. Pure BiFeO3 was produced using an optimized rapid liquid calcination process where the powder was rapidly heated to 880C, heated for 30 min, then rapidly quenched to room temperature. In addition to using the RLC method, it was also necessary to add 2.5 wt% excess Bi2O3 to control Bi volatility as well as 1 wt% Nb2O5 and Na2CO3 powders to stabilize the pure BiFeO3 phase. This powder was used to produce .9NaNbO3-.1BiFeO3 using the Perovskite method. It was found that the secondary phase was still present in the Perovskite method ceramics, which had a Wrec = 2.82 J/cm3, Eb = 320 kV/cm and η = 75.9%.

Rutgers University Community Repository (Rutgers University)
Affordable and clean energy
Ferroelectric and Piezoelectric Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon