Recovery of Potential-Induced Degradation in Polycrystalline Silicon Photovoltaic Modules by Reverse-Bias-Pulse Voltage

The recovery performance from potential-induced degradation (PID) in p-type-based polycrystalline silicon (poly-Si) photovoltaic (PV) modules by the reverse-bias-pulse voltage (VRBP) method has been investigated. This method requires only an external low reverse-bias-pulse voltage between −10 V and −20 V. Further, the VRBP method can be operated at room temperature. The time interval between pulses in the VRBP method is one of the critical factors for a short-term recovery of the module from the PID within 10 minutes. Furthermore, the temperature rise for the VRBP method during the recovery process remains below 100°C. The reasons for these advantages of the VRBP method compared with the conventional recovery method and the reverse DC method are discussed from the viewpoints of using pulsed bias and of the magnitude of the applied electric field during the recovery process.

Authors

Institutions

Publication Details

Journal
MATERIALS TRANSACTIONS
Published
2026-11-24
DOI
https://doi.org/10.2320/matertrans.mt-m2026038
Primary Topic
Silicon and Solar Cell Technologies
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Recovery of Potential-Induced Degradation in Polycrystalline Silicon Photovoltaic Modules by Reverse-Bias-Pulse Voltage

Yasushi Sobajima, Naing Lin Htun, Shingo Hashimoto, Norimitsu Yoshida
MATERIALS TRANSACTIONS
Silicon and Solar Cell Technologies
article

Recovery of Potential-Induced Degradation in Polycrystalline Silicon Photovoltaic Modules by Reverse-Bias-Pulse Voltage

Yasushi Sobajima, Naing Lin Htun, Shingo Hashimoto, Norimitsu Yoshida
article en

Abstract

The recovery performance from potential-induced degradation (PID) in p-type-based polycrystalline silicon (poly-Si) photovoltaic (PV) modules by the reverse-bias-pulse voltage (VRBP) method has been investigated. This method requires only an external low reverse-bias-pulse voltage between −10 V and −20 V. Further, the VRBP method can be operated at room temperature. The time interval between pulses in the VRBP method is one of the critical factors for a short-term recovery of the module from the PID within 10 minutes. Furthermore, the temperature rise for the VRBP method during the recovery process remains below 100°C. The reasons for these advantages of the VRBP method compared with the conventional recovery method and the reverse DC method are discussed from the viewpoints of using pulsed bias and of the magnitude of the applied electric field during the recovery process.

MATERIALS TRANSACTIONSVol. 67(12)
Gifu University (JP)
Silicon and Solar Cell Technologies
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon