Flexural behavior of reinforced concrete beams incorporating graphene oxide: a preliminary experimental investigation and microstructural evaluation

Under flexural loading, microcracks in the tensile zone of reinforced concrete (RC) beams can grow and coalesce into larger cracks. Graphene oxide (GO) may help control this process by promoting cement hydration and bridging microcracks. This study investigated the flexural behavior of M20-grade RC beams incorporating GO at 0.02–0.06 wt.% by mass of​cement. Eighteen beams were tested under four-point bending in six groups of three, and microstructural characterization was used to help interpret the observed response. Ultimate and first-crack loads were compared at the specimen level using one-way analysis of variance (ANOVA) and Tukey’s honestly significant difference (HSD) test. Each dosage was represented by one batch.Stiffness, apparent yield deflection, apparent displacement ductility and energy absorption were derived from the averaged load–deflection curve of each group. The microstructure was examined by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDAX), X-ray diffraction (XRD) and Fourier-transform infrared spectroscopy (FTIR). Under the present four-point bending configuration, GO0.04 gave the highest measured peak load (106 ± 4.2 kN, + 55.9% relative to the control) and the highest energy absorbed up to 30 mm deflection (about + 53%), together with the finest and most closely spaced cracks. GO0.05 and GO0.06 were the stiffest (secant stiffness at 75% of the peak load increased by approximately 113% and 152%, respectively, relative to the control) and had the highest apparent displacement ductility indices (7.1 and 8.0 vs. 4.2).​ These indices were influenced by the small apparent yield deflections and should be interpreted accordingly; their peak loads were lower (71 and 84 kN), which may be consistent with GO agglomeration at higher dosages, although batch, anchorage and shear–flexure effects cannot be excluded. The measured first-crack loads (12.1–19.4 kN) partially overlapped the cracking-load range estimated using IS 456:2000 (15–21 kN). All measured peak loads were below the theoretical first-yield load of the tension steel (approximately 132 kN), suggesting that the bars may have remained below yield. Bar strain and slip were not measured. The microstructural observations are consistent with GO-assisted C–S–H nucleation and a denser hydration-product morphology. Measured peak loads were 64–97% of the design-level IS 456:2000 flexural prediction; insufficient development length of the straight tension bars is considered a likely contributor, and the peak loads reflect combined flexure, bond–anchorage and shear–flexure behaviour rather than pure flexural capacity. With n = 3 specimens from a single batch per group, averaged-curve parameters and no cyclic or durability testing, the findings are indicative and require independent validation.

Authors

Institutions

Publication Details

Journal
Scientific Reports
Published
2026-11-24
DOI
https://doi.org/10.1038/s41598-026-79407-z
Primary Topic
Structural Behavior of Reinforced Concrete
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Flexural behavior of reinforced concrete beams incorporating graphene oxide: a preliminary experimental investigation and microstructural evaluation

Jayaprakash Sridhar, Paul Oluwaseun Awoyera, Olaolu George Fadugba, Kalaiselvi Subramani et al.
4 links
Scientific Reports
Structural Behavior of Reinforced Concrete
article

Flexural behavior of reinforced concrete beams incorporating graphene oxide: a preliminary experimental investigation and microstructural evaluation

Jayaprakash Sridhar, Paul Oluwaseun Awoyera, Olaolu George Fadugba, Kalaiselvi Subramani, Balaji Shanmugam, P. S. Sathish Kumar
article en

Abstract

Under flexural loading, microcracks in the tensile zone of reinforced concrete (RC) beams can grow and coalesce into larger cracks. Graphene oxide (GO) may help control this process by promoting cement hydration and bridging microcracks. This study investigated the flexural behavior of M20-grade RC beams incorporating GO at 0.02–0.06 wt.% by mass of​cement. Eighteen beams were tested under four-point bending in six groups of three, and microstructural characterization was used to help interpret the observed response. Ultimate and first-crack loads were compared at the specimen level using one-way analysis of variance (ANOVA) and Tukey’s honestly significant difference (HSD) test. Each dosage was represented by one batch.Stiffness, apparent yield deflection, apparent displacement ductility and energy absorption were derived from the averaged load–deflection curve of each group. The microstructure was examined by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDAX), X-ray diffraction (XRD) and Fourier-transform infrared spectroscopy (FTIR). Under the present four-point bending configuration, GO0.04 gave the highest measured peak load (106 ± 4.2 kN, + 55.9% relative to the control) and the highest energy absorbed up to 30 mm deflection (about + 53%), together with the finest and most closely spaced cracks. GO0.05 and GO0.06 were the stiffest (secant stiffness at 75% of the peak load increased by approximately 113% and 152%, respectively, relative to the control) and had the highest apparent displacement ductility indices (7.1 and 8.0 vs. 4.2).​ These indices were influenced by the small apparent yield deflections and should be interpreted accordingly; their peak loads were lower (71 and 84 kN), which may be consistent with GO agglomeration at higher dosages, although batch, anchorage and shear–flexure effects cannot be excluded. The measured first-crack loads (12.1–19.4 kN) partially overlapped the cracking-load range estimated using IS 456:2000 (15–21 kN). All measured peak loads were below the theoretical first-yield load of the tension steel (approximately 132 kN), suggesting that the bars may have remained below yield. Bar strain and slip were not measured. The microstructural observations are consistent with GO-assisted C–S–H nucleation and a denser hydration-product morphology. Measured peak loads were 64–97% of the design-level IS 456:2000 flexural prediction; insufficient development length of the straight tension bars is considered a likely contributor, and the peak loads reflect combined flexure, bond–anchorage and shear–flexure behaviour rather than pure flexural capacity. With n = 3 specimens from a single batch per group, averaged-curve parameters and no cyclic or durability testing, the findings are indicative and require independent validation.

Scientific Reports
Prince Mohammad bin Fahd University (SA), Federal University of Technology (NG), Kabale University (UG), Sona College of Technology (IN), GMR Institute of Technology (IN), GITAM University (IN)
Industry, innovation and infrastructure
Structural Behavior of Reinforced Concrete
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon