Engineering sustainable concrete with waste glass powder and recycled PET spiral fibers: experimental, microstructural and exploratory data-driven insights

This study evaluates M30 concrete incorporating waste glass powder (WGP) and recycled polyethylene terephthalate (PET) spiral fibers, with PEG-400 used as an internal-curing agent in the modified mixtures. WGP replacement levels of 0%, 20%, 40%, and 60% were investigated, while a single PET-fiber dosage of 0.6% was tested in the 20% WGP mixture; this dosage was selected for the present experimental program and is not claimed to be an optimized dosage because no multi-level PET optimization study was conducted. The 28-day compressive strength increased from 28.88 MPa for G0 to 33.11 MPa for G20 and 35.11 MPa for G20F, corresponding to 15% and 22% increases, respectively, relative to G0. The reported 28-day flexural strength of G20F was 7.37 MPa, or 146% above G0; this large increase is interpreted cautiously because replicate counts and statistical variability are not reported in the present dataset. Durability indicators including water absorption, sorptivity, and RCPT showed lower values for the 20% WGP mixtures. The sulphuric-acid results, however, did not show a uniform improvement: G20 had a slightly lower mass loss than G0 but a slightly higher strength loss. SEM observations and EDAX Ca/Si ratios are therefore interpreted as qualitative/supporting evidence rather than direct proof of additional C–S–H formation or matrix densification. An exploratory XGBoost/SHAP analysis is retained only as a data-interpretation exercise; because the original workflow included target-derived variables and a limited number of experimental mix designs, its reported predictive accuracy should not be interpreted as evidence of generalizable prediction. Overall, the experimental results indicate that 20% WGP was the highest-performing WGP level among those tested, while the effect of PET and PEG-400 should be interpreted within the stated experimental controls and limitations.

Authors

Institutions

Publication Details

Journal
Scientific Reports
Published
2026-11-24
DOI
https://doi.org/10.1038/s41598-026-74845-1
Primary Topic
Recycled Aggregate Concrete Performance
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Engineering sustainable concrete with waste glass powder and recycled PET spiral fibers: experimental, microstructural and exploratory data-driven insights

Sachin S. Salunkhe, Lenka Čepová, T. Udhaya Kumar, M. Vinod Kumar et al.
3 links
Scientific Reports
Recycled Aggregate Concrete Performance
article

Engineering sustainable concrete with waste glass powder and recycled PET spiral fibers: experimental, microstructural and exploratory data-driven insights

Sachin S. Salunkhe, Lenka Čepová, T. Udhaya Kumar, M. Vinod Kumar, D. Thangaraj
article en

Abstract

This study evaluates M30 concrete incorporating waste glass powder (WGP) and recycled polyethylene terephthalate (PET) spiral fibers, with PEG-400 used as an internal-curing agent in the modified mixtures. WGP replacement levels of 0%, 20%, 40%, and 60% were investigated, while a single PET-fiber dosage of 0.6% was tested in the 20% WGP mixture; this dosage was selected for the present experimental program and is not claimed to be an optimized dosage because no multi-level PET optimization study was conducted. The 28-day compressive strength increased from 28.88 MPa for G0 to 33.11 MPa for G20 and 35.11 MPa for G20F, corresponding to 15% and 22% increases, respectively, relative to G0. The reported 28-day flexural strength of G20F was 7.37 MPa, or 146% above G0; this large increase is interpreted cautiously because replicate counts and statistical variability are not reported in the present dataset. Durability indicators including water absorption, sorptivity, and RCPT showed lower values for the 20% WGP mixtures. The sulphuric-acid results, however, did not show a uniform improvement: G20 had a slightly lower mass loss than G0 but a slightly higher strength loss. SEM observations and EDAX Ca/Si ratios are therefore interpreted as qualitative/supporting evidence rather than direct proof of additional C–S–H formation or matrix densification. An exploratory XGBoost/SHAP analysis is retained only as a data-interpretation exercise; because the original workflow included target-derived variables and a limited number of experimental mix designs, its reported predictive accuracy should not be interpreted as evidence of generalizable prediction. Overall, the experimental results indicate that 20% WGP was the highest-performing WGP level among those tested, while the effect of PET and PEG-400 should be interpreted within the stated experimental controls and limitations.

Scientific Reports
Vel Tech Rangarajan Dr. Sagunthala R&D Institute of Science and Technology (IN), VSB - Technical University of Ostrava (CZ), Saveetha University (IN), Gazi University (TR)
European Commission, Ministerstvo Školství, Mládeže a Tělovýchovy
Responsible consumption and production, Industry, innovation and infrastructure
Recycled Aggregate Concrete Performance
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon