Effect of layer thickness on hot cracking in JBK-75 austenitic stainless steel fabricated by laser powder bed fusion

JBK-75, a precipitation-hardened Fe–29Ni–14Cr austenitic stainless steel, is a candidate alloy for liquid-hydrogen rocket-engine components fabricated by laser powder bed fusion (PBF-LB); however, hot cracking hinders its application. In this study, cracks in JBK-75 built with layer thicknesses of 30 and 60 µm were quantified under ten combinations of laser power, scan speed and hatch distance, and the cracking mechanism was examined using scanning electron microscopy, electron backscattered diffraction (EBSD), electron probe microanalysis, and equilibrium and Scheil–Gulliver calculations with Thermo-Calc. The crack length density ranged from 1.06 to 2.34 mm/mm 2, and approximately 80% of the 442 measured cracks were hot cracks. Under identical scan parameters, the crack length density at 60 µm was 1.4–1.6 times that at 30 µm, mainly because the cracks were longer rather than more numerous. The crack length density decreased with increasing volumetric energy density E at 60 µm but showed no clear dependence at 30 µm; thus, E alone could not explain the layer-thickness effect. The crack examined by EBSD propagated along a high-angle grain boundary (HAGB); HAGBs accounted for 82.3% of all boundaries, and Ti and C, and weakly B, were enriched along the cracks. Thermodynamic calculations showed that TiC is the only phase crystallizing with the liquid, that Ti and B are enriched in the residual liquid, and that under Scheil conditions, 1% liquid persists to approximately 480 K below the equilibrium temperature. Cracking was minimized on the high-energy side, where porosity increases, indicating that densification and crack suppression require different process windows.

Authors

Institutions

Publication Details

Journal
Research Square
Published
2026-11-24
DOI
https://doi.org/10.21203/rs.3.rs-11677293/v1
Primary Topic
Additive Manufacturing Materials and Processes
Type
preprint
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
preprint

Effect of layer thickness on hot cracking in JBK-75 austenitic stainless steel fabricated by laser powder bed fusion

Tadachika Nakayama, Sukhdeep Singh, Magnus Neikter, Wataru Mita et al.
3 links
Research Square
Additive Manufacturing Materials and Processes
preprint

Effect of layer thickness on hot cracking in JBK-75 austenitic stainless steel fabricated by laser powder bed fusion

Tadachika Nakayama, Sukhdeep Singh, Magnus Neikter, Wataru Mita, Kota Kadoi
preprint en

Abstract

JBK-75, a precipitation-hardened Fe–29Ni–14Cr austenitic stainless steel, is a candidate alloy for liquid-hydrogen rocket-engine components fabricated by laser powder bed fusion (PBF-LB); however, hot cracking hinders its application. In this study, cracks in JBK-75 built with layer thicknesses of 30 and 60 µm were quantified under ten combinations of laser power, scan speed and hatch distance, and the cracking mechanism was examined using scanning electron microscopy, electron backscattered diffraction (EBSD), electron probe microanalysis, and equilibrium and Scheil–Gulliver calculations with Thermo-Calc. The crack length density ranged from 1.06 to 2.34 mm/mm 2, and approximately 80% of the 442 measured cracks were hot cracks. Under identical scan parameters, the crack length density at 60 µm was 1.4–1.6 times that at 30 µm, mainly because the cracks were longer rather than more numerous. The crack length density decreased with increasing volumetric energy density E at 60 µm but showed no clear dependence at 30 µm; thus, E alone could not explain the layer-thickness effect. The crack examined by EBSD propagated along a high-angle grain boundary (HAGB); HAGBs accounted for 82.3% of all boundaries, and Ti and C, and weakly B, were enriched along the cracks. Thermodynamic calculations showed that TiC is the only phase crystallizing with the liquid, that Ti and B are enriched in the residual liquid, and that under Scheil conditions, 1% liquid persists to approximately 480 K below the equilibrium temperature. Cracking was minimized on the high-energy side, where porosity increases, indicating that densification and crack suppression require different process windows.

Research Square
University West (SE), Nagaoka University of Technology (JP), The University of Osaka (JP)
Additive Manufacturing Materials and Processes
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon