Mechanical Properties and Microscopic Mechanism of Butyl Rubber Sealing Materials Under Multiple Aging Conditions

The mechanical properties and microstructure of butyl rubber sealant materials were systematically analyzed under high-temperature (40–80 °C), low-temperature (−20 °C), and UV-accelerated aging conditions. Tensile bonding strength, elongation at break, Shore hardness and compressive stress at 20% strain were tested for specimens at different aging periods. Raman spectroscopy and scanning electron microscopy (SEM) were employed to characterize the evolution of molecular structure and surface morphology during aging. Performance retention rates were calculated using non-aged specimens as a common reference, and statistical analysis was conducted via one-way analysis of variance (ANOVA). Results indicate that high-temperature aging markedly reduces tensile bonding strength of butyl rubber: tensile bonding strength decreases by approximately 90.2% at 80 °C compared to the non-aged state, while elongation at break drops by about 80.6%. As temperature increases, thermal oxidation leads to chain scission and reduced unsaturation. Under low-temperature conditions (−20 °C), tensile performance slightly improves, and the molecular structure remains highly stable within 56 days. UV aging primarily causes surface damage; after 35 days of aging, tensile bonding strength decreases by only about 10.9% compared to the non-aged condition, with minimal overall degradation in macroscopic mechanical properties. This study characterizes the chemical and physical aging mechanisms under the three aging conditions, proposes qualitative failure warning indicators, and reveals decoupling phenomena under low-temperature conditions. These findings provide a reference for durability design and material selection in sealing applications.

Authors

Institutions

Publication Details

Journal
Processes
Published
2026-11-24
DOI
https://doi.org/10.3390/pr14233770
Primary Topic
Polymer Science and Applications
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Mechanical Properties and Microscopic Mechanism of Butyl Rubber Sealing Materials Under Multiple Aging Conditions

Xiaoxiang Wei, Yu Hao Feng, Chengjing Xiao, Xizheng Chang et al.
2 links
Processes
Polymer Science and Applications
article

Mechanical Properties and Microscopic Mechanism of Butyl Rubber Sealing Materials Under Multiple Aging Conditions

Xiaoxiang Wei, Yu Hao Feng, Chengjing Xiao, Xizheng Chang, Zhenhua Su, Wenwei Li
article en

Abstract

The mechanical properties and microstructure of butyl rubber sealant materials were systematically analyzed under high-temperature (40–80 °C), low-temperature (−20 °C), and UV-accelerated aging conditions. Tensile bonding strength, elongation at break, Shore hardness and compressive stress at 20% strain were tested for specimens at different aging periods. Raman spectroscopy and scanning electron microscopy (SEM) were employed to characterize the evolution of molecular structure and surface morphology during aging. Performance retention rates were calculated using non-aged specimens as a common reference, and statistical analysis was conducted via one-way analysis of variance (ANOVA). Results indicate that high-temperature aging markedly reduces tensile bonding strength of butyl rubber: tensile bonding strength decreases by approximately 90.2% at 80 °C compared to the non-aged state, while elongation at break drops by about 80.6%. As temperature increases, thermal oxidation leads to chain scission and reduced unsaturation. Under low-temperature conditions (−20 °C), tensile performance slightly improves, and the molecular structure remains highly stable within 56 days. UV aging primarily causes surface damage; after 35 days of aging, tensile bonding strength decreases by only about 10.9% compared to the non-aged condition, with minimal overall degradation in macroscopic mechanical properties. This study characterizes the chemical and physical aging mechanisms under the three aging conditions, proposes qualitative failure warning indicators, and reveals decoupling phenomena under low-temperature conditions. These findings provide a reference for durability design and material selection in sealing applications.

ProcessesVol. 14(23)
China Three Gorges Corporation (China) (CN), Changjiang Water Resources Commission (CN), Yangtze River Pharmaceutical Group (China) (CN), Changjiang River Scientific Research Institute (CN), China Yangtze Power Co., Ltd. (China) (CN)
National Natural Science Foundation of China, China Yangtze Power
Polymer Science and Applications
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon