Investigation of transient multi-indicator in thermal and exergy assessment of yttrium barium zirconate coatings for aluminium–silicon diesel pistons

Diesel engine pistons experience non-uniform and cyclic thermal loading, and excessive crown heating raises the temperature of the aluminium substrate. Coating selection based only on steady temperature reduction overlooks transient heat penetration, coating-side thermal loading and the exergy carried by heat across the crown. In this study, a three-dimensional transient finite element model of an aluminium–silicon diesel piston, with crown loading derived from Diesel-RK, was used to compare an uncoated piston with five ceramic top coats of 0.1–0.5 mm on a 0.1 mm nickel–chromium–aluminium bond coat. Against twenty measured temperatures of an uncoated piston, the model gave a mean absolute error of 3.32 K. At the common thickness of 0.3 mm, yttrium barium zirconate (YBZ) gave the strongest substrate shielding. Under a cold-initialised high-load step with cycle-mean gas-side conditions, it lowered the maximum substrate temperature by 48.87 K, reduced the cumulative convective crown heat transfer over 0–300 s by 25.52% and produced the longest top-coat-to-substrate thermal lag, 15.2 s. Cumulative crown exergy transfer decreased by 11.91% and gas-to-crown exergy destruction by 53.78%. When the crank-angle waveform was resolved, the gas-facing YBZ surface cycled by 149.3 K, whereas the buried NiCrAl/Al–Si interface varied by less than 0.1 K. Thicker YBZ coatings improved substrate protection but raised the top-coat temperature and the temperature difference across the ceramic; all five thicknesses were Pareto non-dominated, so the preferred thickness depends on allowable coating-side limits. The results provide a thermal screening basis for piston coatings, while mechanical integrity and durability require separate assessment.

Authors

Institutions

Publication Details

Journal
Case Studies in Thermal Engineering
Published
2026-11-24
DOI
https://doi.org/10.1016/j.csite.2026.108750
Primary Topic
High-Temperature Coating Behaviors
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Investigation of transient multi-indicator in thermal and exergy assessment of yttrium barium zirconate coatings for aluminium–silicon diesel pistons

Muhammad Bilal Nutkani, Taqi Ahmad Cheema, Cheol Woo Park, Ali Usman et al.
Case Studies in Thermal Engineering
High-Temperature Coating Behaviors
article

Investigation of transient multi-indicator in thermal and exergy assessment of yttrium barium zirconate coatings for aluminium–silicon diesel pistons

Muhammad Bilal Nutkani, Taqi Ahmad Cheema, Cheol Woo Park, Ali Usman, Shah Nawaz Khan, Daniyal Amir
article en

Abstract

Diesel engine pistons experience non-uniform and cyclic thermal loading, and excessive crown heating raises the temperature of the aluminium substrate. Coating selection based only on steady temperature reduction overlooks transient heat penetration, coating-side thermal loading and the exergy carried by heat across the crown. In this study, a three-dimensional transient finite element model of an aluminium–silicon diesel piston, with crown loading derived from Diesel-RK, was used to compare an uncoated piston with five ceramic top coats of 0.1–0.5 mm on a 0.1 mm nickel–chromium–aluminium bond coat. Against twenty measured temperatures of an uncoated piston, the model gave a mean absolute error of 3.32 K. At the common thickness of 0.3 mm, yttrium barium zirconate (YBZ) gave the strongest substrate shielding. Under a cold-initialised high-load step with cycle-mean gas-side conditions, it lowered the maximum substrate temperature by 48.87 K, reduced the cumulative convective crown heat transfer over 0–300 s by 25.52% and produced the longest top-coat-to-substrate thermal lag, 15.2 s. Cumulative crown exergy transfer decreased by 11.91% and gas-to-crown exergy destruction by 53.78%. When the crank-angle waveform was resolved, the gas-facing YBZ surface cycled by 149.3 K, whereas the buried NiCrAl/Al–Si interface varied by less than 0.1 K. Thicker YBZ coatings improved substrate protection but raised the top-coat temperature and the temperature difference across the ceramic; all five thicknesses were Pareto non-dominated, so the preferred thickness depends on allowable coating-side limits. The results provide a thermal screening basis for piston coatings, while mechanical integrity and durability require separate assessment.

Case Studies in Thermal EngineeringVol. 88
Kyungpook National University (KR), Ghulam Ishaq Khan Institute of Engineering Sciences and Technology (PK), Cardiff University (GB)
Kyungpook National University, Ministry of Education, National Research Foundation of Korea, Ministry of Education, India, Ministry of Science and ICT, South Korea
Affordable and clean energy
High-Temperature Coating Behaviors
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon