Evaluation of YOLOv8 instance segmentation variants for surface porosity evaluation in WAAM-CMT 308L beads

Surface porosity is an essential quality indicator in wire arc additive manufacturing (WAAM). However, developing large labelled inspection datasets is challenging due to the high costs associated with experimentation. This research introduces a post-process optical inspection methodology designed to segment and quantify surface pores on WAAM-CMT 308L single beads deposited on a 304L substrate. A comprehensive factorial design comprising 32 beads (4×4×2) was produced, with each bead being captured in a high-resolution image. To address the limited number of bead images and enhance sensitivity to small pore features, each full-bead image was cropped to a bead region of interest and divided into overlapping patches for training, while evaluation was conducted at the bead level to prevent spatial leakage. Five YOLOv8 instance-segmentation variants (v8n/s/m/l/x) were assessed using Accuracy, mAP50, and mAP50-95 on full-bead images. YOLOv8n achieved the highest accuracy (0.9915), whereas YOLOv8l achieved the highest mAP50 (0.6157). YOLOv8x achieved the highest mAP50-95 (0.3949), indicating the strongest segmentation performance among the evaluated variants when averaged across multiple intersection-over-union thresholds. Therefore, YOLOv8x was selected for the final surface porosity quantification stage, where mask localization quality is particularly important for pore area estimation. Comparison with manual measurements on three representative beads yielded a mean absolute error (MAE) of 2.50 percentage points and a root mean square error (RMSE) of 3.08 percentage points. These findings demonstrate the potential of the proposed optical inspection workflow for automated surface porosity assessment in WAAM-CMT single beads, while highlighting the importance of selecting segmentation models according to the evaluation metric most relevant to the intended application.

Authors

Institutions

Publication Details

Journal
Engineering Research Express
Published
2026-11-23
DOI
https://doi.org/10.1088/2631-8695/aec550
Primary Topic
Industrial Vision Systems and Defect Detection
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Evaluation of YOLOv8 instance segmentation variants for surface porosity evaluation in WAAM-CMT 308L beads

Farhat Zemzemi, Hédi Hamdi, Oussama Trad, Souhaila Khalfallah et al.
Engineering Research Express
Industrial Vision Systems and Defect Detection
article

Evaluation of YOLOv8 instance segmentation variants for surface porosity evaluation in WAAM-CMT 308L beads

Farhat Zemzemi, Hédi Hamdi, Oussama Trad, Souhaila Khalfallah, Ated BEN KHALIFA
article en

Abstract

Surface porosity is an essential quality indicator in wire arc additive manufacturing (WAAM). However, developing large labelled inspection datasets is challenging due to the high costs associated with experimentation. This research introduces a post-process optical inspection methodology designed to segment and quantify surface pores on WAAM-CMT 308L single beads deposited on a 304L substrate. A comprehensive factorial design comprising 32 beads (4×4×2) was produced, with each bead being captured in a high-resolution image. To address the limited number of bead images and enhance sensitivity to small pore features, each full-bead image was cropped to a bead region of interest and divided into overlapping patches for training, while evaluation was conducted at the bead level to prevent spatial leakage. Five YOLOv8 instance-segmentation variants (v8n/s/m/l/x) were assessed using Accuracy, mAP50, and mAP50-95 on full-bead images. YOLOv8n achieved the highest accuracy (0.9915), whereas YOLOv8l achieved the highest mAP50 (0.6157). YOLOv8x achieved the highest mAP50-95 (0.3949), indicating the strongest segmentation performance among the evaluated variants when averaged across multiple intersection-over-union thresholds. Therefore, YOLOv8x was selected for the final surface porosity quantification stage, where mask localization quality is particularly important for pore area estimation. Comparison with manual measurements on three representative beads yielded a mean absolute error (MAE) of 2.50 percentage points and a root mean square error (RMSE) of 3.08 percentage points. These findings demonstrate the potential of the proposed optical inspection workflow for automated surface porosity assessment in WAAM-CMT single beads, while highlighting the importance of selecting segmentation models according to the evaluation metric most relevant to the intended application.

Engineering Research Express
University of Monastir (TN), Université de Lyon (FR), École Nationale d'Ingénieurs de Gabès (TN), University of Sousse (TN)
Industrial Vision Systems and Defect Detection
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon