Effect of Calcination Temperature on the Structure and NH3-SCR Performance of 8Fe2O3-5CeO2-40MnO2/TiO2 Catalysts

The NH3-SCR performance of Fe-Ce-Mn/TiO2 catalysts depends on calcination temperature. To examine this effect at fixed composition, 8Fe2O3-5CeO2-40MnO2/TiO2 was prepared by co-precipitation and calcined at 200, 300, 400 or 500 °C for 4 h. The 400 °C sample provided the widest temperature range with at least 90% NO conversion (129–390 °C), reached a maximum of 99.17% and had the lowest apparent activation energy (55.78 kJ mol−1). It showed favorable N2 selectivity and retained the highest conversion in the SO2 and combined SO2/H2O resistance tests. XRD, N2 physisorption, microscopy, XPS, NH3-TPD and H2-TPR results showed that calcination altered pore development, particle aggregation and surface properties. At lower calcination temperatures, less developed pores and greater aggregation limited the exposure of supported metal species and coincided with poorer SCR performance. By 400 °C, pore development and particle dispersion had improved, accompanied by greater surface metal exposure, NH3 uptake and overall reducibility. Further heating to 500 °C increased aggregation and reduced surface metal fractions and total NH3 uptake without improving activity. Calcination at 400 °C for 4 h gave the best overall performance in the series.

Authors

Institutions

Publication Details

Journal
Catalysts
Published
2026-11-23
DOI
https://doi.org/10.3390/catal16121053
Primary Topic
Catalytic Processes in Materials Science
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Effect of Calcination Temperature on the Structure and NH3-SCR Performance of 8Fe2O3-5CeO2-40MnO2/TiO2 Catalysts

Xue Bian, Zhongshuai Jia, Jiaqi Li, Bin Zhang et al.
Catalysts
Catalytic Processes in Materials Science
article

Effect of Calcination Temperature on the Structure and NH3-SCR Performance of 8Fe2O3-5CeO2-40MnO2/TiO2 Catalysts

Xue Bian, Zhongshuai Jia, Jiaqi Li, Bin Zhang, Xuewen Mu, Yuming Yang, Guomin Hong, Yu Chen, Zhicheng Wang
article en

Abstract

The NH3-SCR performance of Fe-Ce-Mn/TiO2 catalysts depends on calcination temperature. To examine this effect at fixed composition, 8Fe2O3-5CeO2-40MnO2/TiO2 was prepared by co-precipitation and calcined at 200, 300, 400 or 500 °C for 4 h. The 400 °C sample provided the widest temperature range with at least 90% NO conversion (129–390 °C), reached a maximum of 99.17% and had the lowest apparent activation energy (55.78 kJ mol−1). It showed favorable N2 selectivity and retained the highest conversion in the SO2 and combined SO2/H2O resistance tests. XRD, N2 physisorption, microscopy, XPS, NH3-TPD and H2-TPR results showed that calcination altered pore development, particle aggregation and surface properties. At lower calcination temperatures, less developed pores and greater aggregation limited the exposure of supported metal species and coincided with poorer SCR performance. By 400 °C, pore development and particle dispersion had improved, accompanied by greater surface metal exposure, NH3 uptake and overall reducibility. Further heating to 500 °C increased aggregation and reduced surface metal fractions and total NH3 uptake without improving activity. Calcination at 400 °C for 4 h gave the best overall performance in the series.

CatalystsVol. 16(12)
Baogang Group (China) (CN), Northeastern University (CN)
Catalytic Processes in Materials Science
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
Effect of Calcination Temperature on the Structure and NH3-SCR Performance of 8Fe2O3-5CeO2-40MnO2/TiO2 Catalysts — Xue Bian, Zhongshuai Jia, et al. · Catalysts (2026) | TGRS Research Map | TGRS