Influence of Fiber Orientation and Laminate Architecture on the Mechanical, Thermal, and Morphological Performance of Rattan Fiber/Epoxy Composites

To investigate the impact of fiber orientation and stacking sequence on the characterization of rattan fiber epoxy composites, eight laminates with fiber orientations and stacking sequences of [0°] 4 , [30°] 4 , [60°] 4 , [90°] 4 , [0°/90°] 2 , [0°/90°] s , [±45°] 2 , and [0°/30°/60°/90°] were fabricated using vacuum bagging method. Mechanical properties, including tensile, flexural, and rockwell hardness; thermal properties, including thermogravimetric and differential scanning calorimetry analysis; Fourier Transform Infrared Spectroscopy; and morphological characteristics were evaluated in this study. The [0°] 4 laminate demonstrated the maximum tensile strength of 18.43 MPa and Young's modulus of 2.77 GPa, while the [90°] 4 laminate demonstrated the lowest tensile strength of 4.87 MPa, indicating that load transmission is strongly dependent on fiber alignment. With a strength of 34.99 MPa, [0°] 4 had the best flexural performance, while the symmetric [0°/90°] s laminate had the greatest flexural modulus of 3.75 GPa, closely followed by [0°] 4 laminate (3.73 GPa). Hardness test results were almost constant between 66–68 HRL, suggesting that fiber orientation had minimal impact. Thermogravimetric analysis revealed multi‐stage degradation, with maximum decomposition temperatures between 370°C–380°C and significant weight loss (40%–55%) taking place between 350°C‐450°C. Glass transition temperatures were found to be between 87°C–89°C using differential scanning calorimetry. Cellulose, lignin, and epoxy functional groups were confirmed by FTIR, while SEM evaluation showed reasonable fiber–matrix wetting along with voids, interfacial debonding, fiber pull‐out, and fiber splitting in all laminates. Finally, the experimental findings of both Young's modulus and flexural modulus were compared with theoretical predictions.

Authors

Institutions

Publication Details

Journal
SPE Polymers
Published
2026-11-23
DOI
https://doi.org/10.1002/pls2.70090
Primary Topic
Natural Fiber Reinforced Composites
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Influence of Fiber Orientation and Laminate Architecture on the Mechanical, Thermal, and Morphological Performance of Rattan Fiber/Epoxy Composites

Md. Abdul Hasib, M.S. Rabbi, Md. Mahmudul Adil, Afnan Hasan et al.
SPE Polymers
Natural Fiber Reinforced Composites
article

Influence of Fiber Orientation and Laminate Architecture on the Mechanical, Thermal, and Morphological Performance of Rattan Fiber/Epoxy Composites

Md. Abdul Hasib, M.S. Rabbi, Md. Mahmudul Adil, Afnan Hasan, Gogan Dhar
article en

Abstract

To investigate the impact of fiber orientation and stacking sequence on the characterization of rattan fiber epoxy composites, eight laminates with fiber orientations and stacking sequences of [0°] 4 , [30°] 4 , [60°] 4 , [90°] 4 , [0°/90°] 2 , [0°/90°] s , [±45°] 2 , and [0°/30°/60°/90°] were fabricated using vacuum bagging method. Mechanical properties, including tensile, flexural, and rockwell hardness; thermal properties, including thermogravimetric and differential scanning calorimetry analysis; Fourier Transform Infrared Spectroscopy; and morphological characteristics were evaluated in this study. The [0°] 4 laminate demonstrated the maximum tensile strength of 18.43 MPa and Young's modulus of 2.77 GPa, while the [90°] 4 laminate demonstrated the lowest tensile strength of 4.87 MPa, indicating that load transmission is strongly dependent on fiber alignment. With a strength of 34.99 MPa, [0°] 4 had the best flexural performance, while the symmetric [0°/90°] s laminate had the greatest flexural modulus of 3.75 GPa, closely followed by [0°] 4 laminate (3.73 GPa). Hardness test results were almost constant between 66–68 HRL, suggesting that fiber orientation had minimal impact. Thermogravimetric analysis revealed multi‐stage degradation, with maximum decomposition temperatures between 370°C–380°C and significant weight loss (40%–55%) taking place between 350°C‐450°C. Glass transition temperatures were found to be between 87°C–89°C using differential scanning calorimetry. Cellulose, lignin, and epoxy functional groups were confirmed by FTIR, while SEM evaluation showed reasonable fiber–matrix wetting along with voids, interfacial debonding, fiber pull‐out, and fiber splitting in all laminates. Finally, the experimental findings of both Young's modulus and flexural modulus were compared with theoretical predictions.

SPE PolymersVol. 8(1)
Chittagong University of Engineering & Technology (BD), Khulna University (BD), Khulna University of Engineering and Technology (BD), Bangladesh Army University of Science and Technology (BD)
Natural Fiber Reinforced Composites
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon