Systemic regulation of depth of discharge mitigates electrochemical-mechanical degradation in 198 Ah Ni-rich lithium-ion batteries
Rapid electrochemical-mechanical degradation bottlenecks nickel-rich layered cathodes. We demonstrate that restricting the depth of discharge to 94% in 198 Ah industrial NCM batteries effectively mitigates severe anisotropic lattice strain. This systemic intervention strongly suppresses impedance escalation and macroscopic swelling, markedly extending cycle life under rigorous fast-charging and practical mixed-charging protocols.
Authors
- Tianyu Zhu (ORCID: https://orcid.org/0000-0003-4690-8586)
- Dong Zhou (ORCID: https://orcid.org/0000-0003-1786-7463)
- Xiaokang Ju (ORCID: https://orcid.org/0000-0002-8840-2244)
- Jun Wang (ORCID: https://orcid.org/0000-0001-9561-5857)
- Zhenjin Liang
- Guohua Zheng
- Yongxin Wang
- Chao Wang
- Rui Liang
- Xuan He
- Hongling Shi
- Qian Wang
Institutions
- Sun Yat-sen University (CN)
- Southern University of Science and Technology (CN)
- Shandong University of Science and Technology (CN)
Publication Details
- Journal
- Chemical Communications
- Published
- 2026-11-23
- DOI
- https://doi.org/10.1039/d6cc05910d
- Primary Topic
- Battery Modeling and Management
- Type
- article
- Field-Weighted Citation Impact
- 0.00