Mechanical, tribological, and corrosion resistance performance of CrN, VN, and CrVN coatings deposited by magnetron sputtering

Binary CrN and VN, and ternary CrVN ceramic coatings were deposited by DC magnetron co-sputtering from single-element targets, with the nitrogen flow (10, 40 and 80 sccm) as the sole variable. XRD showed the binary ceramics to be highly reactive gas flow-sensitive – CrN evolving from a metallic-Cr/Cr 2 N mixture toward cubic CrN, and VN degrading toward a quasi-amorphous state at 80 sccm – whereas the ternary CrVN retained a well-defined FCC structure across the whole range. SEM-EDS showed that all coatings are nitrogen-deficient (N/Me = 0.35–0.68) and that the loss of long-range order in the binaries coincides with oxygen uptake (O/Me up to ≈ 0.8), which the CrVN coatings, grown at the highest metal flux, largely avoid (O/Me ≤ 0.14). Increasing the nitrogen flow softened all systems (CrN hardest, ≈ 15 GPa; VN softest, ≈ 8 GPa; CrVN intermediate). The CrVN coatings combined competitive hardness with by far the best adhesion (Lc3 up to ≈ 9 N vs ≈ 4 N for the binaries), the lowest friction coefficient (≈ 0.45), the most stable, near-neutral open-circuit potential and the slowest development of corrosion products under SO 2 exposure. Linear polarization showed, however, that nobility does not rank the corrosion kinetics: the apparent corrosion current densities of CrVN (≈ 4–6 µA cm −2 ) were comparable to those of CrN, and the lowest value (≈ 1.2 µA cm −2 ) was obtained for the insulating CrN_80 oxynitride. Within each series, the electrical resistivity and the hardness followed the oxygen content of the coatings rather than their Cr/V ratio, and adhesion was highest for the thickest (CrVN) coatings. Co-sputtering Cr and V therefore yields the best balance of hardness, adhesion, friction and electrochemical stability, making CrVN a promising multifunctional protective coating.

Authors

Institutions

Publication Details

Journal
Materials Today Communications
Published
2026-11-24
DOI
https://doi.org/10.1016/j.mtcomm.2026.116745
Primary Topic
Metal and Thin Film Mechanics
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Mechanical, tribological, and corrosion resistance performance of CrN, VN, and CrVN coatings deposited by magnetron sputtering

Dan Cristea, Cătălin Croitoru, A.V. Surdu, D. Cristea et al.
1 links
Materials Today Communications
Metal and Thin Film Mechanics
article

Mechanical, tribological, and corrosion resistance performance of CrN, VN, and CrVN coatings deposited by magnetron sputtering

Dan Cristea, Cătălin Croitoru, A.V. Surdu, D. Cristea, A. Crisbasan, C. Croitoru
article en

Abstract

Binary CrN and VN, and ternary CrVN ceramic coatings were deposited by DC magnetron co-sputtering from single-element targets, with the nitrogen flow (10, 40 and 80 sccm) as the sole variable. XRD showed the binary ceramics to be highly reactive gas flow-sensitive – CrN evolving from a metallic-Cr/Cr 2 N mixture toward cubic CrN, and VN degrading toward a quasi-amorphous state at 80 sccm – whereas the ternary CrVN retained a well-defined FCC structure across the whole range. SEM-EDS showed that all coatings are nitrogen-deficient (N/Me = 0.35–0.68) and that the loss of long-range order in the binaries coincides with oxygen uptake (O/Me up to ≈ 0.8), which the CrVN coatings, grown at the highest metal flux, largely avoid (O/Me ≤ 0.14). Increasing the nitrogen flow softened all systems (CrN hardest, ≈ 15 GPa; VN softest, ≈ 8 GPa; CrVN intermediate). The CrVN coatings combined competitive hardness with by far the best adhesion (Lc3 up to ≈ 9 N vs ≈ 4 N for the binaries), the lowest friction coefficient (≈ 0.45), the most stable, near-neutral open-circuit potential and the slowest development of corrosion products under SO 2 exposure. Linear polarization showed, however, that nobility does not rank the corrosion kinetics: the apparent corrosion current densities of CrVN (≈ 4–6 µA cm −2 ) were comparable to those of CrN, and the lowest value (≈ 1.2 µA cm −2 ) was obtained for the insulating CrN_80 oxynitride. Within each series, the electrical resistivity and the hardness followed the oxygen content of the coatings rather than their Cr/V ratio, and adhesion was highest for the thickest (CrVN) coatings. Co-sputtering Cr and V therefore yields the best balance of hardness, adhesion, friction and electrochemical stability, making CrVN a promising multifunctional protective coating.

Materials Today CommunicationsVol. 58
Transylvania University of Brașov (RO)
Metal and Thin Film Mechanics
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon
Mechanical, tribological, and corrosion resistance performance of CrN, VN, and CrVN coatings deposited by magnetron sputtering — Dan Cristea, Cătălin Croitoru, et al. · Materials Today Communications (2026) | TGRS Research Map | TGRS