Comparative Study of Fused Deposition Modeling-Manufactured Polylactic Acid (PLA) Screws and Commercial Polyether Ether Ketone (PEEK) and Poly(L-lactide-co-D,L-lactide) (PLDLLA) Implants for Orthopedic Fixation: An In Vivo Assessment

Orthopedic fixation requires implants that combine mechanical stability with geometries adapted to anatomical and surgical requirements. The biodegradability, tunable mechanical properties, and geometric versatility of polylactic acid (PLA) make it attractive for patient-specific orthopedic implants; however, the long-term in vivo response of Fused Deposition Modeling (FDM)-manufactured PLA screws remains insufficiently understood. This study evaluated the postoperative response from early healing through eight months, comparing FDM-fabricated PLA screws with clinically established polyether ether ketone (PEEK) and poly(L-lactide-co-D,L-lactide) (PLDLLA) screws. PLA screws were fabricated layer by layer by FDM, enabling application-specific geometries, including fine thread pitches and customized features. The materials were characterized by dynamic mechanical analysis (DMA) and Fourier-transform infrared spectroscopy (FTIR), while computed tomography (CT) and histology evaluated structural integrity and the bone–implant interface over time. All implants maintained structural integrity throughout eight months without premature degradation. PLA exhibited progressive new bone formation and partial tissue integration, with increasing bone maturation over time. PEEK showed predominantly fibrointegrative healing early, followed by increased mature bone densification at long-term implantation. PLDLLA promoted rapid tissue integration and dense mature cortical bone formation from the early stage. Overall, FDM enabled the fabrication of biodegradable PLA screws with application-specific and potentially patient-tailored geometries, supporting their potential for osteoconductive orthopedic fixation.

Authors

Institutions

Publication Details

Journal
Biomolecules
Published
2026-11-23
DOI
https://doi.org/10.3390/biom16121701
Primary Topic
Bone Tissue Engineering Materials
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Comparative Study of Fused Deposition Modeling-Manufactured Polylactic Acid (PLA) Screws and Commercial Polyether Ether Ketone (PEEK) and Poly(L-lactide-co-D,L-lactide) (PLDLLA) Implants for Orthopedic Fixation: An In Vivo Assessment

Victor Manuel Orozco-Carmona, Nadia Karina Portillo Ortiz, Arturo Luévano-González, Gregorio Vázquez-Olvera et al.
Biomolecules
Bone Tissue Engineering Materials
article

Comparative Study of Fused Deposition Modeling-Manufactured Polylactic Acid (PLA) Screws and Commercial Polyether Ether Ketone (PEEK) and Poly(L-lactide-co-D,L-lactide) (PLDLLA) Implants for Orthopedic Fixation: An In Vivo Assessment

Victor Manuel Orozco-Carmona, Nadia Karina Portillo Ortiz, Arturo Luévano-González, Gregorio Vázquez-Olvera, Reyna Guadalupe Sánchez-Duarte, Roberto Gómez Batres, Edmundo Berumen-Nafarrate, A. Martinez-García, Karime Carrera-Gutiérrez, Brianda Aragón-García, Carolina Valdez-Velázquez, Jesus Manuel Maynez-Villalobos, David Chung-Arceo, Edith Sáenz-Flores, Lorenzo Buenabad, Brissa Aylin Gómez-Salgado
article en

Abstract

Orthopedic fixation requires implants that combine mechanical stability with geometries adapted to anatomical and surgical requirements. The biodegradability, tunable mechanical properties, and geometric versatility of polylactic acid (PLA) make it attractive for patient-specific orthopedic implants; however, the long-term in vivo response of Fused Deposition Modeling (FDM)-manufactured PLA screws remains insufficiently understood. This study evaluated the postoperative response from early healing through eight months, comparing FDM-fabricated PLA screws with clinically established polyether ether ketone (PEEK) and poly(L-lactide-co-D,L-lactide) (PLDLLA) screws. PLA screws were fabricated layer by layer by FDM, enabling application-specific geometries, including fine thread pitches and customized features. The materials were characterized by dynamic mechanical analysis (DMA) and Fourier-transform infrared spectroscopy (FTIR), while computed tomography (CT) and histology evaluated structural integrity and the bone–implant interface over time. All implants maintained structural integrity throughout eight months without premature degradation. PLA exhibited progressive new bone formation and partial tissue integration, with increasing bone maturation over time. PEEK showed predominantly fibrointegrative healing early, followed by increased mature bone densification at long-term implantation. PLDLLA promoted rapid tissue integration and dense mature cortical bone formation from the early stage. Overall, FDM enabled the fabrication of biodegradable PLA screws with application-specific and potentially patient-tailored geometries, supporting their potential for osteoconductive orthopedic fixation.

BiomoleculesVol. 16(12)
Universidad Autónoma de Guadalajara (MX), Autonomous University of Chihuahua (MX), Universidad de Guadalajara (MX), Sonora Institute of Technology (MX), Centro de Investigación en Materiales Avanzados (MX), Centro Universitario de Chihuahua (MX)
Universidad Autónoma de Chihuahua
Bone Tissue Engineering Materials
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon