Surface and Interface Engineering of Sb2S3/ZnO Heterostructures Fabricated by CBD and ALD for Thin-Film Photovoltaic Applications

Sb2S3/ZnO heterostructures were fabricated by chemical bath deposition (CBD) of Sb2S3 for 30, 35, and 40 min, yielding thicknesses of 252, 311, and 387 nm, followed by vacuum annealing at 350 °C and atomic layer deposition (ALD) of a 44 nm ZnO layer at 200 °C. The influence of the absorber deposition time on the structural, morphological, optical, and photoelectrical properties was evaluated. X-ray diffraction confirmed orthorhombic Sb2S3, hexagonal ZnO, and a secondary Sb2O3 phase whose fraction increased from 9.0% (30 min) to 14.7% (40 min). Rietveld refinement showed that the Sb2S3 fraction increased from 28.5% (30 min) to 43.4% (35 min) and remained constant at 40 min, while the ZnO fraction decreased from 62.5% to 41.9%. Williamson–Hall analysis yielded crystallite sizes of 29.1, 36, and 20.1 nm and dislocation densities of 1.17, 0.77, and 2.46 × 10–3 nm–2 for the 30, 35, and 40 min samples, respectively. SEM revealed wheat-like grains at 30 and 40 min and rosette-like clusters with coarser, elongated grains at 35 min. The 35 min sample also exhibited the highest Zn and lowest O contents by EDS. The effective band gaps were 2.3, 1.6, and 2.1 eV, respectively, governed by the Sb2S3 fraction, crystalline quality, and oxide content. All heterostructures exhibited a photoresponse that decreased with increasing absorber thickness, with the 30 min sample showing the highest photocurrent. Overall, the Sb2S3 (35 min)/ZnO heterostructure provided the best compromise, combining the highest crystalline quality and the lowest effective band gap with a photocurrent only slightly lower than that of the 30 min sample, highlighting its potential for low-cost thin-film photovoltaic devices.

Authors

Institutions

Publication Details

Journal
ACS Omega
Published
2026-11-23
DOI
https://doi.org/10.1021/acsomega.6c08955
Primary Topic
Chalcogenide Semiconductor Thin Films
Type
article
Field-Weighted Citation Impact
0.00

Funders

Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Surface and Interface Engineering of Sb2S3/ZnO Heterostructures Fabricated by CBD and ALD for Thin-Film Photovoltaic Applications

Daniel Arturo Acuña Leal, Cristian Gómez-Rodríguez, Linda Viviana García-Quiñonez, María Isabel Mendivil Palma et al.
ACS Omega
Chalcogenide Semiconductor Thin Films
article

Surface and Interface Engineering of Sb2S3/ZnO Heterostructures Fabricated by CBD and ALD for Thin-Film Photovoltaic Applications

Daniel Arturo Acuña Leal, Cristian Gómez-Rodríguez, Linda Viviana García-Quiñonez, María Isabel Mendivil Palma, Roberto Martínez Ronquillo, Daniel Fernández González
article en

Abstract

Sb2S3/ZnO heterostructures were fabricated by chemical bath deposition (CBD) of Sb2S3 for 30, 35, and 40 min, yielding thicknesses of 252, 311, and 387 nm, followed by vacuum annealing at 350 °C and atomic layer deposition (ALD) of a 44 nm ZnO layer at 200 °C. The influence of the absorber deposition time on the structural, morphological, optical, and photoelectrical properties was evaluated. X-ray diffraction confirmed orthorhombic Sb2S3, hexagonal ZnO, and a secondary Sb2O3 phase whose fraction increased from 9.0% (30 min) to 14.7% (40 min). Rietveld refinement showed that the Sb2S3 fraction increased from 28.5% (30 min) to 43.4% (35 min) and remained constant at 40 min, while the ZnO fraction decreased from 62.5% to 41.9%. Williamson–Hall analysis yielded crystallite sizes of 29.1, 36, and 20.1 nm and dislocation densities of 1.17, 0.77, and 2.46 × 10–3 nm–2 for the 30, 35, and 40 min samples, respectively. SEM revealed wheat-like grains at 30 and 40 min and rosette-like clusters with coarser, elongated grains at 35 min. The 35 min sample also exhibited the highest Zn and lowest O contents by EDS. The effective band gaps were 2.3, 1.6, and 2.1 eV, respectively, governed by the Sb2S3 fraction, crystalline quality, and oxide content. All heterostructures exhibited a photoresponse that decreased with increasing absorber thickness, with the 30 min sample showing the highest photocurrent. Overall, the Sb2S3 (35 min)/ZnO heterostructure provided the best compromise, combining the highest crystalline quality and the lowest effective band gap with a photocurrent only slightly lower than that of the 30 min sample, highlighting its potential for low-cost thin-film photovoltaic devices.

ACS Omega
Universidad Veracruzana (MX), Universidad de Oviedo (ES), Universidad Autónoma de Nuevo León (MX)
Agencia Estatal de Investigación
Chalcogenide Semiconductor Thin Films
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon