Continuous evaluation of bending strain tolerance along a hundred meter class REBCO tape

Strain tolerance of REBa2Cu3O7-δ (REBCO, RE: rare earth) coated conductors is a key factor in the performance and reliability of high field superconducting magnets. This study evaluates the longitudinal uniformity of the critical current (Ic) response to bending in two approximately 98 m sections along a single, uncut 460 m commercial REBCO tape. The sections were continuously bent at room temperature using rollers with radius from 20 to 6 mm, followed by magnetization based Ic measurements at 77 K. Ic degraded progressively as the bending radius decreased with the REBCO layer on the outside of the bend, whereas no detectable degradation occurred with the REBCO layer on the inside over the investigated range. Weibull model analysis indicated a narrow distribution of bending tolerance over most of the tested length, together with rare early degrading regions estimated to occupy approximately 0.1% of that length. These regions did not coincide with the pre-existing Ic drops, suggesting that the pre-existing low Ic regions did not systematically exhibit lower tolerance to tensile bending. Magnetic field profiles showed that the early degradation generally initiated at the tape width edges. The average irreversible bending strain estimated from the beam bending formula was 0.32–0.44%, lower than the 0.47–0.51% obtained in 77 K tensile tests on straight samples. Surface profile measurements, cross sectional observations, and elastoplastic simulations showed that Poisson induced anticlastic deformation increased the local longitudinal strain at the tape width edges. In addition, accounting for the increased strain at the tape edges shifted the inferred irreversible strain range to 0.43–0.60%, substantially overlapping the 0.47–0.51% range obtained from the 77 K tensile tests. The results demonstrate high longitudinal uniformity within the tested tape sections and indicate that local edge strain enhancement is an important factor in interpreting bending induced degradation.

Authors

Institutions

Publication Details

Journal
Superconductor Science and Technology
Published
2026-11-23
DOI
https://doi.org/10.1088/1361-6668/aec59e
Primary Topic
Superconducting Materials and Applications
Type
article
Field-Weighted Citation Impact
0.00
Controls
|||
ALL TIME
JAN
FEB
MAR
APR
MAY
JUN
JUL
AUG
SEP
OCT
NOV
article

Continuous evaluation of bending strain tolerance along a hundred meter class REBCO tape

Gen Nishijima, Toshio Yamazaki, 上田克英, Yoshinori Yanagisawa et al.
Superconductor Science and Technology
Superconducting Materials and Applications
article

Continuous evaluation of bending strain tolerance along a hundred meter class REBCO tape

Gen Nishijima, Toshio Yamazaki, 上田克英, Yoshinori Yanagisawa, Peifeng Gao, Takanobu KISS, Kensuke Kobayashi, Yasuaki Takeda, Shoichi Yokoyama, Renzhong Piao, Mamoru Hamada, Shaoyu Zheng, Michitaka Ono
article en

Abstract

Strain tolerance of REBa2Cu3O7-δ (REBCO, RE: rare earth) coated conductors is a key factor in the performance and reliability of high field superconducting magnets. This study evaluates the longitudinal uniformity of the critical current (Ic) response to bending in two approximately 98 m sections along a single, uncut 460 m commercial REBCO tape. The sections were continuously bent at room temperature using rollers with radius from 20 to 6 mm, followed by magnetization based Ic measurements at 77 K. Ic degraded progressively as the bending radius decreased with the REBCO layer on the outside of the bend, whereas no detectable degradation occurred with the REBCO layer on the inside over the investigated range. Weibull model analysis indicated a narrow distribution of bending tolerance over most of the tested length, together with rare early degrading regions estimated to occupy approximately 0.1% of that length. These regions did not coincide with the pre-existing Ic drops, suggesting that the pre-existing low Ic regions did not systematically exhibit lower tolerance to tensile bending. Magnetic field profiles showed that the early degradation generally initiated at the tape width edges. The average irreversible bending strain estimated from the beam bending formula was 0.32–0.44%, lower than the 0.47–0.51% obtained in 77 K tensile tests on straight samples. Surface profile measurements, cross sectional observations, and elastoplastic simulations showed that Poisson induced anticlastic deformation increased the local longitudinal strain at the tape width edges. In addition, accounting for the increased strain at the tape edges shifted the inferred irreversible strain range to 0.43–0.60%, substantially overlapping the 0.47–0.51% range obtained from the 77 K tensile tests. The results demonstrate high longitudinal uniformity within the tested tape sections and indicate that local edge strain enhancement is an important factor in interpreting bending induced degradation.

Superconductor Science and Technology
Kyushu University (JP), National Institute for Materials Science (JP), Superconductor Technologies (United States) (US), RIKEN (JP), Lanzhou University (CN)
Superconducting Materials and Applications
AI Navigator

Ask Laika to Summarize, Analyze, and Connect papers live on the map.

Summarize Papers & Methodologies

Extract key findings, datasets, and comparative methods across publications.

Benchmark Rankings & Visual Analytics

Rank top research institutions, authors, funders, topics, and journals by Field-Weighted Citation Impact (FWCI) and paper volume with instant charts.

Connect Distant Disciplines

Bridge topological clusters on the map to find hidden collaborative intersections.

Laika access coming soon